Feature Article
NPE News Wrap-up: Resin Dryers
At least 16 companies introduced new dryers at the big show in Chicago. The new
models span a range of drying technologies, but most sport features that save
space and cost and make the dryers simpler and more reliable.
|
|
By Matthew H. Naitove
|
|
|
| Learn More |
| Company Info |
|
AEC Inc.
Wood Dale Ill.
(630) 595-1060
Bry-Air Systems
Sunbury, Ohio
(877) 4BRYAIR
Canam Manufactured Products Inc.
Surrey, B.C.
(604) 888-7699
Comet Automation Systems
Dayton, Ohio
(937) 296-9166
Conair
Pittsburgh, PA
(412) 312-6000
Dri-Air Industries, Inc.
East Windsor, Conn.
(860) 627-5110
Foremost Machine Builders, Inc.
Fairfield, N.J.
(973) 227-0700
Maguire Products, Inc.
Aston, Pa.
(888) 459-2412
Matsui America, Inc.
Elk GroveVillage, Ill.
(847) 290-9680
Motan Inc.
Plainwell, Mich.
(269) 685-1050
Novatec, Inc.
Baltimore
(410) 789-4811
Process Control Corp.
Atlanta
(770) 449-8810
Sterling Material Processing, div. of Sterling, Inc.
Milwaukee
(414) 354-0970
Thoreson-McCosh Inc.
Troy, Mich.
(248) 362-0960
Universal Dynamics, Inc.
Woodbridge, Va.
(703) 491-2191
Walton/Stout, Inc.
Lithonia, Ga.
(800) 822-8633
Wittmann Inc.
Torrington. Conn.
(860) 496-9603
|
|
ResinWorks from Conair is a highly flexible, customizable new system of multiple drying hoppers on a single sled. It permits quick material changes and precise control of individual hoppers.
|
Resin dryers were the most numerous new entries in materials-handling equipment
at NPE. They included every possible size and type, from conventional desiccant
models to hot-air, vacuum, and compressed-air types—with or without drying
membrane. Suppliers have focused their attention on reducing energy usage, maintenance,
and up-front cost while also making the dryers more self-regulating and foolproof.
Among the benefits most commonly cited for the new models are smaller footprints,
easier cleanout, all-stainless construction, and increased drying speed and
efficiency. A number have loading and conveying integrated with the dryer. New
controls range from ultra-simple to full-featured, but even the latter are said
to be easier to use than ever. Touchscreens dominate, and several units can
automatically drop temperature and air flow when a drying hopper is not in use
to prevent overdrying or degrading the resin and wasting energy.
Membrane dryers
NPE 2003 saw the arrival of the first competitors for the NovaDrier that Novatec
introduced at NPE 2000. It was a new type of dryer that uses heated compressed
air and a special moisture-removal membrane that is quite different from a standard
desiccant. There is no separate regeneration cycle, since the membrane purges
itself automatically and continuously. This simple design has no moving parts
and is said to save energy and dry very quickly. It even works for PET, according
to Novatec. However, it appears to be limited to small and medium sizes because
the special membrane is expensive. Novatec has sold about 700 of these patented
dryers.
|
All-stainless hoppers are used on new portable drying/conveying systems like
AECs Nomad II (left) and Universal Dynamics GS model (below).
|
|
This year, both AEC and Sterlings new Material Handling Div. introduced
compressed-air dryers with a reverse-osmosis membrane. AECs
ACM Series and Sterlings SMD Series come in models with capacities of
30 and 60 cfm (30 and 60 lb/hr). They cost the same as standard dryers but are
more compact, suiting them to machine mounting. They reportedly achieve 40
F dewpoint and heat up to 300 F (400 F optional), so theyre not suitable
for higher-temperature resins like PET, say AEC sources.
Motan offers an optional coalescent membrane with its new LCA compressed-air
dryers, described in the next section. The membrane is standard on the companys
new Micro Dryer, whose glass-bodied hopper holds about 1 lb.
Meanwhile, Novatec came out with two new control options for its NovaDriers.
The Energy Saver monitors the difference between hopper inlet and outlet temperatures
with an optional thermocouple. If the hopper is empty or resin flow stops for
any reason, the Delta T becomes zero and the controller shuts off
the compressed air and booster heater. If the hopper returns to active use,
the air and heat come back on automatically. This option is also available on
desiccant dryers that have the NovaTouch touchpanel PLC.
The Moisture Manager option, already available on NovaTouch-equipped desiccant
dryers, is for critical medical and automotive parts that require precise dewpoint
control. For example, it is said to prevent overdrying of nylons and certain
polyesters. The user dials in the desired dewpoint, and the unit senses the
dewpoint of the air leaving the hopper. The Moisture Manager varies the proportion
of fresh compressed air to recirculated air to maintain the dewpoint target
within ±1° F, the company claims.
More non-desiccant dryers
Another type of dryer that first appeared at NPE 2000 is the vacuum dryer from
Maguire Products. Maguire has sold around 500 of these Low Pressure Dryers (LPDs),
and at NPE 2003, Maguire unveiled the largest model to date, the LPD-1000. It
handles 1000 lb/hr, five times the capacity of the next largest size.This is
the first LPD model suitable for large-volume PET processors. Because it uses
only vacuum to pull moisture out of the resin, the LPD reportedly requires only
20% as much energy and one-sixth as much drying time as standard dryers. It
also permits much lower drying temperatures—for example, 300 F for PET
vs. the usual 350 F.
|
Motan brought out its first compressed-air dryers, including this LCA 30, which
has an optional coalescent membrane.
|
Theres more news in compressed-air dryers, as well. Both AEC and Sterling
introduced straight compressed-air dryers similar to their new models that have
a membrane. These models (AECs AC Series and Sterlings SCD Series)
reduce the drying-air dewpoint by 20° F.
Comet Automation Systems is now the exclusive distributor of the ERD Baby, Junior,
and Senior lines of compressed-air dryers from Fasti-Austria. They achieve 40
F dewpoints and come in sizes from 2 to 3000 lb/hr.
Motan brought out its first compressed-air dryers, Models LCA 15 and 30, which
are aimed at low throughputs. They have bin capacities of 15 and 30 lb, respectively,
and use 2.5 to 9 cfm of compressed air. These throat-mounted models reportedly
can achieve dewpoints of 13 F (or 40 F with the optional membrane).
The Autoload Div. of Universal Dynamics showed a new and much larger series
of compressed-air dryers called AutoDry II. The previous range went up to 120-lb
hopper capacity. The new units go from 200 to 800 lb. Heating capacity is to
400 F.
Thoreson-McCosh has a new hot-air dryer that reportedly can process ABS at 20
to 30 lb/hr and PET at 60 lb/hr. It uses heat pipes to distribute heat rapidly
and evenly (±1° F) from top to bottom. It reportedly gets material
up to drying temperature in 30 min or less. (The heat-pipe approach is also
used in hot-air Speedryers from Canam Manufactured Products.)
|
Matsuis new MJ3 portable dryer/loader is more efficient, more compact,
and more economical than previous models.
|
Also new is Matsuis model MGD, its first hot-air dryer/loader combination.
It has a stainless hopper and line-purge capability.
Desiccant dryers galore
New desiccant dryers, from micro to maxi, were also plentiful at NPE. A number
of them came with upgraded controls and/or integral loading/conveying systems.
- AECs new AD Series of mini cabinet dryers has a dual-bed, closed-loop
design and off-the-shelf microprocessor controls with autotuning
PID temperature control as standard. Drying temperatures go up to 300 F (400
F optional). Enclosed cabinet style provides maximum safety. Blower capacities
are 15, 30, or 60 cfm.
AEC showed its largest desiccant central dryer to date, the new AD-3000, which
has 3000 cfm of air flow and AP-1 PLC control with touchscreen. Gas-fired heaters
are optional.
New Nomad II portable drying systems from AEC integrate dry-air conveying on
a single cart. The all-stainless systems include an AD Series desiccant dryer
and touchscreen PLC controls. They can serve one or two machines.
Also new from AEC is the AP-2 dryer control with Allen-Bradley PLC and touchscreen.
It shows set and actual temperatures and actual dewpoint as well as the high-level
alarm setting. An auto-shutdown sequence is preprogrammed.
- Bry-Air Systems has broadened its line with the new EZ-Dry system, which has
a desiccant rotor instead of discrete beds and a fluted instead of beaded desiccant
media. Its said to allow greater air velocity to pass through the desiccant,
resulting in faster drying from a smaller, lighter unit (capacities up to 600
lb/hr). Continuously rotating desiccant eliminates dewpoint spikes. Also, the
fluted media reportedly lasts twice as long as typical beaded media and costs
less to replace.
Available on the EZ Dry and all Bry-Air models is the new optional Smart Dry
controller. The microprocessor-based diagnostic controller has a seven-day timer
and ability to maintain a set dewpoint. It monitors dewpoint, process and regeneration
temperatures, return air temperatures, and various alarm functions. It can also
be monitored remotely.
- The latest from Comet Automation Systems is the FCD-10100 honeycomb desiccant
dryer with integral hopper loader and dry-air conveying capability. It has microprocessor
control, 100-lb/hr capacity, and ability to serve two machines.
- Conair brought out the D Series of small dryers for up to 100 lb/hr. These
unusually compact models resemble a mold-temperature controller in shape and
size (35 x 17 x 27 in.). They use Conairs standard indexing desiccant
carousel. Prices start at $2800 and go up according to three levels of optional
controls. The basic DC control has a simple LED display of set or actual process
and regeneration temperatures. It also indicates a high-temperature alarm. The
mid-level DC-1 control has simultaneous LED display of set and actual temperatures,
various alarms, an alarm history to help with diagnostics, and auto-start countdown
timer. The full-featured DC-2 control has an LCD display of operating status,
set-up parameters, diagnostics, alarm log, event log, and other information.
An extra LED display lets the user give added visibility to any critical parameter.
It also has a membrane keypad and field-bus communications.
|
Dri-Airs new Micro Dryer is aimed atmicromolding and dries as little
as 5 g.
|
Conairs major debut in drying was the ResinWorks central drying/blending/conveying
system. Each is custom configured from a menu of standard components. Up to
five drying hoppers are mounted on a single sled together with heaters,
controls, dry-air manifolds, and purge valves. Each hopper can be sized for
multi-machine/long-run use or single-machine/short-run operation. Multiple sleds
can be assembled for large installations. The ResinWorks system can also incorporate
a gaylord or bag feed station and/or gravimetric blenders. Conveying controls
can be simple or sophisticated as needed.
The resin-distribution manifold has an electrical proofing system to ensure
that the right material goes to the right machine. To prevent contamination,
a single conveying line is dedicated to each machine. The line is purged (with
dry air if necessary) after each conveying cycle. So material changes can be
made in 10 min or less by simply changing the mechanical connection at the manifold
and cleaning out the hopper on the machine.
|
Some new compact units like Sterlings STT40 have dryer sections resembling a small mold-temperature controller.
|
Special features of the system included the ability to isolate each drying hopper
in terms of heating and air flow. A new proprietary valve adjustment system
allows precise calibration of air flow to each hopper—something difficult
to accomplish until now, according to Conair. And once set, the air flow adjustment
can be locked to prevent fiddling. Also, a special lever can be actuated to
positively shut off air and heat to a bin. Other new features include oversized
access doors that permit easier cleanout and a reportedly unique external purge
valve for dried materials. It is said to be simpler, more compact, and more
economical than standard designs.
The aim of the system is to provide complete flexibility to convey any
material to any machine at any time. ResinWorks is expected to appeal
particularly to processors of engineering materials who make several material
changes per week per machine.
- New entries from Dri-Air Industries span the full range of sizes. Its new Micro
Dryer for micromolding dries as little as 5 g up to 5 lb. The compact, lightweight,
and inexpensive unit (around $2100) uses shop compressed air together with dual
desiccant beds. Air flow can be adjusted from 0.5 to 3 cfm to provide dewpoints
to 40 F. At the opposite end of the size scale, Dri-Air has extended its
line of large, multi-bed dryers to include the model HP4-X-750, which processes
750 lb/hr. Dri-Air also expanded the RH series of drying hoppers up to 2000-lb
capacity.
In addition, Dri-Air has a new dryer for two-shot molding: It dries two resins
with independent control of temperature and time. Also new is the Med-X Series
of four-bed desiccant dryers for medical molding. It has HEPA-filtered air and
a seamless stainless-steel hopper that is polished to a mirror finish. A handheld
vacuum-cleaner accessory is standard on this model. Cleanliness is also the
hallmark of Dri-Airs new dryer for CD/DVD molding. It is also fully polished
inside but has no cleanout door since it is dedicated to running one material.
A built-in Pelletron deduster keeps the resin free of fines and dust.
|
Wittmanns Drymax 30 is its first machine-mounted dryer.
|
Other news from Dri-Air includes an integral hopper loader for use in closed-loop
loading systems with its PD Series portable dryers. It uses a single blower
to convey material up to 200 ft to the drying hopper and from the dryer to the
molding machine. That eliminates the need for a loader motor on the press.
New microprocessor controls for Dri-Airs multi-hopper banks offer independent
control of time and temperature at up to eight hoppers. The hoppers can be of
different sizes and can dry even partial loads of as little as 2 lb without
overdrying, the company claims.
- Foremost Machine Builders was one of several firms introducing new drying hoppers
with a solid instead of perforated spreader cone at the bottom to permit easier
cleaning.
- Matsui America came out with a whole new Plas-Aid line of auxiliary equipment,
which includes the Multi-Jet 3 (MJ3) portable dryer/loader. Its honeycomb desiccant
rotor is said to be more efficient than the previous design used on Matsuis
DMZ dryer. This allows the unit to be more compact and more competitively priced.
The integral loader can feed two machines. New standard features include all-stainless
interior, solid-state relays, and line purging with dry air.
The improved rotor and solid-state relays are also used on the new model DMZ-2
dryer without a loader. It is also less expensive than the previous DMZ model.
|
Thoreson McCosh puts heat pipes inside the aluminum fins of its new hot-air
dryer to distribute heat evenly.
|
- Motan has two new central drying products. Its Luxor A twin-tower models have
a new touchscreen control panel that shows data trends, alarm logs, and Help
screens for alarms. The optional Drying Organizer calculates material throughput
and automatically reduces the temperature to prevent overdrying if material
is not being used. It also displays a wait alarm if material is
under-dried. One new option is control via the Pocketnet handheld PDA, which
communicates with the dryers Mitsubishi PLC via wireless internet connection.
Also new is the Luxor 200S, the first of a line of simple, low-cost dryers with
stationary twin towers and PLC (see PT, May 03, p. 104).
- As reported previously, Process Control Corp. re-entered the dryer market after
nearly 20 years with its D Series of fixed and portable desiccant models. (PT,
May 03, p. 105).
- Sterling Material Handling has a new STT Series of desiccant dryers for central
and beside-the-machine use. They have modular design, nonferrous construction
(including stainless heaters), and integrally mounted process heater, which
eliminates heat loss through transfer piping. Controls regulate blower speed
to prevent overdrying when not running at full capacity. Multiple hoppers can
be individually controlled.
- Thoreson-McCosh has improved its T-D Series desiccant dryer by adding
temperature sensors at the top and bottom of the hopper. If the hopper is running
too slowly, the Delta T drops and the hopper will be shut down automatically.
Also new is the ability to set the air flow in cfm digitally from the control
panel rather than adjusting a valve by hand.
|
Solid-cone hoppers are easier to clean than perforated cones. (Photo: Foremost)
|
- Modular design is basic to the new GS twin-bed dryers from Universal Dynamics.
They are 20% less expensive than the firms UDC dryers and also simpler
to control. Additional temperature sensors in the desiccant towers are said
to provide better control of regeneration. These dryers use new TSC insulated
drying hoppers, which have a solid-cone bottom for easy cleaning and smooth,
all-stainless interiors with no pellet-retaining lip or ledges. These hoppers
are also less expensive than previous models. GS dryers ship in three to five
days. Sizes are 30 to 150 cfm, and combined drying/conveying versions are available.
- Two new Ener$ave options from Walton/Stout recapture heat that
is normally wasted. ERS-II is an air-to-air heat exchanger that uses hot, wet
process air to preheat air coming back to the hopper from the desiccant dryer.
Retrofittable on other brands of dryers, ERS-II is said to save as much as 25%
of energy use.
The second Ener$ave approach sends a small amount of process air through a newly
regenerated desiccant bed, cooling the bed and recapturing the heat. This not
only eliminates a temperature spike from the regenerated bed but also saves
about 5% in energy use by recapturing excess heat that is usually removed by
a cooling coil and thrown away.
- Wittmann introduced its first machine-mounted dryer, the Drymax 30. This twin-bed
unit for up to 35 lb/hr heats to 320 F and achieves 40 F dewpoint. Its
oversized desiccant beds combine larger desiccant volume with lower air velocity
for more efficient drying. The beds are removable, allowing the media to be
changed off-line.
Also new from Wittmann is the Drymax 100 Series portable desiccant dryer with
two hoppers and SmartFlow valves. It runs up to 155 lb/hr. SmartFlow valves
replace manually adjusted air flappers; the valves automatically adjust air
flow and heat to the hoppers based on sensor readings. By monitoring the Delta
T between incoming and outgoing air in each hopper, the valve can shut off air
flow and heat to a hopper that experiences low throughput or can increase flow
and heat to a hopper that is in high demand.
Wittmann also redesigned its line of CDD continuous desiccant-wheel dryers (250