Resin Pricing–January 2005

[ Previous Page | Recycled Resin Prices ]

Market Prices Effective Mid-Dec A

 RESIN GRADEb
¢/LB
¢/CU INc
 

 ABS

 

 
 
 MED IMPACT
 80 - 90 Prices Went Up 
 3.0 - 3.4 Prices Went Up 
 
 HI IMPACT
 85 - 95 Prices Went Up 
 3.2 - 3.6 Prices Went Up 
 
 X-HI IMPACT
 95 - 105 Prices Went Up 
 3.6 - 4.0 Prices Went Up 
 
 HI HEAT
 85 - 95  
 3.2 - 3.6  
 
 PIPE
 80 - 110 Prices Went Up 
 3.0 - 4.2 Prices Went Up 
 
 SHEET
 90 - 110 Prices Went Up 
 3.4 - 4.2 Prices Went Up 
 
 TRANSPARENT
 125 - 165  
 4.9 - 6.4  
 
 FITTINGS
 85 - 115 Prices Went Up 
 3.2 - 4.3 Prices Went Up 
 
 PLATING
 95 - 105  
 3.5 - 3.9  
 
 FLAME RET
 120 - 140 Prices Went Up 
 4.6 - 5.9 Prices Went Up 
 
 STRUCT FM
 83 - 97  
 3.6 - 4.3  
 
 10% GLASS
 125 - 140  
 5.0 - 5.6  
 
 30% GLASS
 116 - 136  
 5.3 - 6.3  
 
 ABS/PC ALLOY
 145 - 180 Prices Went Up 
 5.5 - 6.8 Prices Went Up 
 
 ABS/PVC ALLOY
 130 - 135  
 5.8 - 6.1  
 
 ABS/NYLON ALLOY
 190  
 7.3  
 


 ACETAL

 

 
 
 HOMOPOL
 130 - 147  
 6.7 - 7.3  
 
 20% GLASS
 160 - 220  
 9.0 - 12.4  
 
 COPOLYMER
 133 - 137  
 6.8 - 7.0  
 
 25% GLASS
 160 - 215  
 9.2 - 12.3  
 


 ACRYLIC

 

 
 
 G-P
 117 - 152 Prices Went Up 
 5.0 - 6.5 Prices Went Up 
 
 IMPACT
 162 - 222 Prices Went Up 
 6.9 - 9.5 Prices Went Up 
 


 ACRYLONITRILE COPOL

 

 
 
 EXTRUSION
 101 - 116  
 4.0 - 4.6  
 
 INJECTION
 120 - 135  
 4.8 - 5.4  
 


 ALKYD

65 - 74  

4.9 - 5.5  
 


 CELLULOSICS

 

 
 
 ACETATE
 187  
 8.6  
 
 CAB
 189  
 8.2  
 
 CAP
 189  
 8.2  
 


 DAP (G-P)

251 - 497  

16.7 - 34.7  
 


 EPOXY

 

 
 
 G-P RESIN
 116 - 126  
 NAd  
 
 COMPOUNDS
   
   
 
 C/B/Te
 123 - 166  
 9.4 - 12.9  
 
 R/C/Df
 208 - 271  
 15.3 - 20.1  
 
 SEMICONDUCTOR
   
   
 
 NOVOLAC
 193 - 228  
 13.1 - 15.9  
 
 ANHYDRIDE
 188 - 268  
 13.9 - 19.2  
 


 EVA

 

 
 
 INJECTION
 46 - 52  
 1.5 - 1.7  
 
 FILM EXTRU
 42 - 49  
 1.4 - 1.6  
 


 EVOH

265  

11.3  
 


 FLUORO-POLYMER

 

 
 
 CTFE
 4500  
 346.6  
 
 ECTFE
 1400 - 1600  
 108.3 - 123.8 
 
 ETFE
 1100 - 1600  
 73.6 - 107.1 
 
 FEP
 925 - 1400  
 71.3 - 107.9 
 
 PFA
 1700 - 2400  
 131.6 - 185.8 
 
 PTFE
 450 - 900  
 34.8 - 69.7  
 
 PVDF
 650 - 800  
 41.4 - 50.9  
 


 IONOMER

 

 
 
 PACKAGING
 127 - 166  
 4.3 - 6.0  
 
 INDUSTRIAL
 150 - 244  
 5.0 - 8.3  
 


 LIQUID-CRYSTAL POLYMERS

 

 
 
 INJECTION MIN FILLED
 690 - 1035  
 44.2 - 72.1  
 
 GLASS FILLED
 695 - 895  
 40 - 52  
 
 CARBON FILLED
 1700 - 2000  
 83.2 - 138.6 
 
 UNFILLED
 1000 - 1200  
 58 - 70  
 
 EXTRUSION UNFILLED
 1200 - 2200  
 60.5 - 110.9 
 


 MELAMINE COMPOUND

90 - 94  

5.5 - 5.6  
 


 MELAMINE/PHENOLIC COMPOUND

75 - 83  

4.5 - 5.0  
 


 NYLON

 

 
 
 TYPE 6
 139 - 159 Prices Went Up 
 5.7 - 6.5 Prices Went Up 
 
 MIN FILLED
 131 - 144 Prices Went Up 
 5.4 - 5.9 Prices Went Up 
 
 30% GLASS
 148 - 173 Prices Went Up 
 6.0 - 7.0 Prices Went Up 
 
 TYPE 66
 153 - 168 Prices Went Up 
 6.3 - 6.9 Prices Went Up 
 
 MIN FILLED
 151 - 159 Prices Went Up 
 6.2 - 6.5 Prices Went Up 
 
 30% GLASS
 142 - 192 Prices Went Up 
 5.8 - 7.9 Prices Went Up 
 
 TYPE 69
 250 - 276  
 9.7 - 10.7  
 
 TYPE 6/10
 286 - 313  
 12.4 - 13.6  
 
 TYPE 612
 400  
 15.3  
 
 30% GLASS
 309 - 311  
 14.7  
 
 40% GLASS
 309  
 14.7  
 
 TYPE 46
 295  
 12.6  
 
 TYPE 11
 329 - 341  
 13.6 - 14.1  
 
 30% GLASS
 331 - 350  
 15.0 - 15.8  
 
 40% GLASS
 347 - 360  
 17.7 - 18.5  
 
 TYPE 12
 318 - 341  
 12.1 - 13.0  
 
 30% GLASS
 327 - 350  
 14.7 - 15.8  
 
 50% GLASS
 299 - 340  
 15.6 - 17.8  
 
 TRANSPARENT AMORPHOUS
 247 - 360  
 10.3 - 15.0  
 


 PHENOLIC MOLD COMP

75  

3.8  
 
 REINFORCED GRADES
 105 - 268  
 6.1 - 16  
 


 POLYAMIDE-IMIDEg

 

 
 
 UNFILLED
 2310 - 3045  
 117.8 - 155.3 
 
 30% GLASS
 2250 - 2985  
 130.4 - 173.0 
 
 30% CARBON FIB.
 3260 - 3950  
 173.6 - 210.5 
 


 POLYARYLATE

200 - 280  

8.8 - 12.3  
 


 POLYARYL SULFONE

440  

21.8  
 


 POLYBUTYLENE

 

 
 
 G-P
 94 - 96  
 3.1  
 
 FILM
 88 - 91  
 2.9  
 
 PIPE
   
   
 
 COLD WATER
 116 - 120  
 3.9 - 4.0  
 
 HOT WATER
 162 - 166  
 5.5 - 5.6  
 


 POLYCARBONATE

 

 
 
 INJECTION
 138 - 165  
 5.9 - 7.0  
 
 20% GLASS
 177 - 190  
 7.6 - 8.2  
 
 30% GLASS
 178 - 217  
 7.6 - 9.3  
 
 EXTRUSION
 145 - 180 Prices Went Up 
 6.3 - 7.8 Prices Went Up 
 
 BLOW MOLD
 155 - 190 Prices Went Up 
 6.7 - 8.2 Prices Went Up 
 
 STRUCT FOAM
 149 - 181  
 6.4 - 7.8  
 
 20% GLASS
 235 - 255  
 10.1 - 11.0  
 
 FR
 166 - 197  
 7.1 - 8.5  
 
 CD
 140 - 200 Prices Went Up 
 6.0 - 8.6 Prices Went Up 
 


 POLYESTER (TP) PBT TYPE

 

 
 
 UNFILLED
 143 - 150  
 6.9  
 
 HI-IMP
 154 - 165  
 7.6  
 
 30% GLASS, FR
 165 - 187  
 10.0  
 
 STRUCT FOAM
 159 - 165  
 NAd  
 


 PET

 

 
 
 BOTTLE (RAILCAR)
 89 - 91 Prices Went Up 
 4.5 - 4.6 Prices Went Up 
 
 MOD PET
   
   
 
 30% GLASS
 132 - 143  
 7.4  
 
 55% GLASS
 148 - 155  
 9.8  
 
 30% GLASS FLAME RET
 147 - 157  
 9.2  
 
 PETG COPOL
 114 - 124  
 5.2 - 5.6  
 
 RESIN GRADEb
¢/LB
¢/CU INc
 


 POLYESTER THERMOSET

 

 
 
 G-P ORTHO
 95 - 105 Prices Went Up 
 NAd  
 
 ISOPHTHALIC
 120 - 130 Prices Went Up 
 NAd  
 
 BIS-A
 160 - 195 Prices Went Up 
 NAd  
 


 PEEK

4400  

231  
 
 30% GLASS
 3300  
 173  
 


 POLYETHERIMIDE

641 - 646  

29.3 - 29.5  
 
 30% GLASS
 526 - 531  
 24.0 - 24.2  
 


 POLYETHERKETONE (PEK)

2950  

130.1  
 
 30% GLASS
 2600  
 153  
 


 POLYETHERSULFONE

350 - 400  

17.2 - 19.7  
 
 30% GLASS
 425 - 525  
 21 - 25.9  
 


 POLYETHYLENE (RAILCAR) LDPE

 

 
 
 G-P MOLDING & EXTRU
 88 - 90 Prices Went Up 
 2.9 - 3.0 Prices Went Up 
 
 INJECTION
 88 - 90 Prices Went Up 
 2.9 - 3.0 Prices Went Up 
 
 LID RESIN
 90 - 92 Prices Went Up 
 3.0 Prices Went Up 
 
 LINER
 88 - 90 Prices Went Up 
 2.9 - 3.0 Prices Went Up 
 
 CLARITY
 87 - 90 Prices Went Up 
 2.9 - 3.0 Prices Went Up 
 
 EXTRU COATG
 89 - 91 Prices Went Up 
 2.9 - 3.0 Prices Went Up 
 
 BLOW MOLD
 90 - 92 Prices Went Up 
 3.0 - 3.2 Prices Went Up 
 


 LLDPE, BUTENE BASED

 

 
 
 G-P MOLDING
 75 - 77 Prices Went Up 
 2.5 - 2.6 Prices Went Up 
 
 FILM
 77 - 79 Prices Went Up 
 2.6 Prices Went Up 
 
 ROTOMOLD
 79 - 81 Prices Went Up 
 2.6 - 2.7 Prices Went Up 
 


 LLDPE, HAO-BASED

 

 
 
 G-P MOLDING
 81 - 83 Prices Went Up 
 2.7 Prices Went Up 
 
 LID RESIN
 87 - 89 Prices Went Up 
 2.9 Prices Went Up 
 
 LINER FILM
 82 - 84 Prices Went Up 
 2.7 - 2.8 Prices Went Up 
 


 HDPE

 

 
 
 G-P INJ MOLD
 77 - 79 Prices Went Up 
 2.6 - 2.7 Prices Went Up 
 
 FILM
 85 - 87 Prices Went Up 
 2.7 - 2.9 Prices Went Up 
 
 BLOW MOLD
 79 - 81 Prices Went Up 
 2.7 - 2.8 Prices Went Up 
 

 HMW-HDPE

 

 
 
 BLOW MOLDING
 87 - 89 Prices Went Up 
 2.9 Prices Went Up 
 
 FILM
 89 - 91 Prices Went Up 
 2.9 - 3.1 Prices Went Up 
 
 PIPE
 93 - 95 Prices Went Up 
 3.2 Prices Went Up 
 


 UHMW-PE

100 - 125  

3.6 - 3.7  
 


 PPE/PPO BASED RESIN

 

 
 
 INJECTION
 180  
 6.8  
 
 20% GLASSh
 283  
 12.3  
 
 30% GLASSh
 291  
 13.3  
 
 EXTRUSIONh
 242  
 9.2  
 
 STRUCT FM
 231  
 NAd  
 


 PPS

 

 
 
 40% GLASS
 340 - 385  
 20 - 23  
 
 55% GLASS/MINERAL
 275 - 295  
 16 - 17.4  
 
 65% GLASS/MINERAL
 215 - 260  
 11 - 14  
 


 POLYPROPYLENE (RAILCAR)

 

 
 
 G-P HOMOPOL INJECTION
 72 - 74 Prices Went Up 
 2.3 Prices Went Up 
 
 EXTRUSION FIBER
 68 - 70 Prices Went Up 
 2.2 - 2.3 Prices Went Up 
 
 PROFILES
 72 - 74 Prices Went Up 
 2.3 - 2.4 Prices Went Up 
 
 RANDOM COPOL
   
   
 
 BLOW MOLDING
 76 - 78 Prices Went Up 
 2.5 Prices Went Up 
 
 FILM
 74 - 76 Prices Went Up 
 2.4 - 2.5 Prices Went Up 
 
 INJECTION
 73 - 75 Prices Went Up 
 2.4 - 2.5 Prices Went Up 
 
 IMPACT COPOL
   
   
 
 MED IMP
 86 - 88 Prices Went Up 
 2.8 - 2.9 Prices Went Up 
 
 HI IMP
 89 - 91 Prices Went Up 
 2.9 Prices Went Up 
 


 POLYSTYRENE (RAILCAR)

 

 
 
 G-P CRYSTAL
 72 - 81  
 2.7 - 3.0  
 
 HI HEAT
 75 - 84  
 2.8 - 3.1  
 
 HIPS
 73 - 82  
 2.7 - 3.1  
 
 SUPER HI IMP
 83 - 90  
 3.1 - 3.4  
 
 FR
 91 - 102  
 3.4 - 3.8  
 
 STRUCT FM (FR)
 95 - 98  
 na  
 


 EPS

 

 
 
 UNMODIFIED
 80 - 83  
 NAd  
 
 MODIFIED
 81 - 85  
 NAd  
 


 POLYSULFONE

432 - 512  

19.3 - 22.9  
 
 10% GLASS 430 20.6
 605 - 612  
 27 - 27.3  
 
 30% GLASS 372 20.01
 557 - 562  
 24.9 - 25  
 


 POLYURETHANE (TP)

 

 
 
 ESTER TYPE
 185 - 255  
 8 - 11  
 
 ETHER TYPE
 245 - 295  
 10.6 - 13  
 


 PU ISOCYANATES

 

 
 
 POLYMERIC MDI
 105 - 115  
 NAd  
 
 80/20 TDI
 110 - 120  
 NAd  
 


 PVC RESIN (RAILCAR)

 

 
 
 G-P HOMOPOL
 45 - 47 Prices Went Up 
 NAd  
 
 PIPE
 43 - 46 Prices Went Up 
 NAd  
 
 FILM
 55 - 57 Prices Went Up 
 NAd  
 
 COPOLYMER FLOORING
 58 - 60  
 NAd  
 
 DISPERSION HOMOPOLY
 57 - 75  
 NAd  
 
 COPOLYMER
 72 - 76  
 NAd  
 
 CPVC PIPE COMPOUND
 119  
 NAd  
 


 PVDC

 

 
 
 EXTRUDABLE
 162  
 NAd  
 


 SILICONES

 

 
 
 MOLD. COMP.
 581 - 640  
 38.1 - 39.3  
 
 SPECIALTY GR.
 891 - 3148  
 NAd  
 
 SILICONE/EPOXY
 339 - 343  
 22.5 - 22.8  
 


 STYRENEACRYLIC

108 - 112  

3.7 - 4.0  
 


 SAN (G-P)

66 - 74  

2.5 - 2.8  
 


 STYRENE MALEIC ANHYDRIDE

 

 
 
 G-P
 110 - 115  
 4.2 - 4.3  
 
 HI IMP
 130 - 140  
 4.2 - 4.5  
 
 FR
 175 - 183  
 6.7 - 7.0  
 


 TP ELASTOMERS

 

 
 
 OLEFINIC
 70 - 76  
 2.4  
 
 POLYAMIDE
 287 - 337  
 10.4 - 12.3  
 
 POLYESTER
 200 - 310  
 8.8 - 13.6  
 
 STYRENIC
 82 - 237  
 2.9 - 8.3  
 


 UREA MOLDING COMPOUND

 

 
 
 BLACK & BROWN
 76  
 3.8  
 
 WHITE & IVORY
 81  
 4.0  
 


 VINYL ESTER

 

 
 
 COR RES
 147  
 NAd  
 
 HEAT & COR RES
 161  
 NAd  
 

KEY: Colored areas indicate pricing activity. An arrow () indicates direction of price change. aTruckload, unless otherwise specified. bUnfilled, natural color, unless otherwise specified. cBased on typical or average density. dNot applicable. eNovolac and anhydride grades for coils, bushings, transformers. fNovolac and anhydride grades for resisitors, capacitors, diodes. gIn quantities of 20,000 lb. h19,800-lb load.

PT Home | Zones | Suppliers | Materials Search | Machinery Search | Latest Issue | Article Search | Resin Prices | Blog | e-Newsletters |Subscribe | Advertise | Contact us

The Definitive Web Resource For Plastics Processors

© 2009 Gardner Publications, Inc