Monomers Push Up Resin Prices


By Lilli Manolis Sherman, Jan H. Schut

print this article Print This Article


[ Resin Pricing Chart ]

Prices of PP, PVC, and PET moved up last month and new price hikes were under way for PE, PP, PS, PVC, and PET.

PE prices up 3¢
Polyethylene prices moved up 3¢/lb in March, bringing the total increase this year to 6¢/lb. Suppliers pushed back their announced 7¢ hike again, this time to May 1. Moreover, the price increase has been modified: Suppliers now want a 7¢/lb increase only for hexene-grade LLDPE, due to tight supplies, and 4¢/lb on all other PE resins.

The London Metal Exchange (LME) short-term futures contract for May in g-p blown film butene LLDPE sold at 53.1¢/lb, up from April’s 52.2¢.

Contributing factors: Ethylene monomer contract prices moved up 1.5¢/lb in March, after remaining flat the previous month. Further price increases are not anticipated soon, as monomer supplies are plentiful.

Meanwhile, domestic PE demand is still relatively lackluster, despite a slight seasonal uptick in the last two months. Exports also appear to have slowed, particularly to Asia. Still, resin capacity utilization is a little above 90%.

Director of market research Cindy Bryan at resin purchasing consultant Resin Technology, Inc. (RTI), Fort Worth, Texas, says current market factors don’t support higher prices. “Processors are still buying as needed, due to the expectation that the price increases won’t go through—or if they do, they will be short-lived,” says Bryan.

PP prices on the way up
Polypropylene prices were slated to move up last month, as suppliers aimed to implement the 4¢/lb hike announced for April 1. It would bring the total increase this year to 9¢/lb. A new price hike of 3¢ was announced for May 1. Meanwhile, LME’s May futures contract for g-p injection-grade homopolymer sold at 58.4¢/lb, up from April’s 52.2¢.

Contributing factors: The major driving force is higher monomer prices. April contract prices rose 4¢/lb and there was talk of possible 1¢ to 2¢ increases for May.

PP demand in the first quarter averaged about 6% higher than the same period last year, with growth of 4% in January and February and a 10% jump in March. But these numbers include exports. Says RTI managing partner Scott Newell, “Minus those exports, domestic demand has been flat at best, if not down a bit.” Resin makers’ capacity utilization is a little above 90%, but that could change, as China has drastically curtailed U.S. resin purchases of as much as 120 million lb/month, according to Newell.

Meanwhile, a mechanical breakdown at Sunoco’s 700-million-lb PP plant in Neal, W.Va., led the company to declare force majeure in mid-April. At press time it was unknown how long it would take to restart operations or what effect this might have on tightening resin supply.

PVC: another 2¢ hike
The March price increase of 3¢/lb for PVC took effect, large processors say. A 3¢ increase announced for April is expected to go through, too, if pipe producers succeed in raising their prices. OxyChem, Georgia Gulf, and Formosa announced a further 3¢ hike for May 1, though Shintech reportedly trimmed that back to 2¢.

Contributing factors: Pipe demand has risen as distributors restock. Window and siding demand hasn’t picked up appreciably. The American Plastics Council’s preliminary figure for PVC resin capacity utilization for March was 88%, up from 86% in February.

PS hike pushed to May
Polystyrene producers got a 4¢/lb increase in March as expected, but pushed a 3¢ hike back from April 1 to May 1. Ineos and Total upsized their May 1 hike to 5¢/lb from 3¢.

Contributing factors: Feedstock prices are again squeezing PS producers. Ethylene monomer went up from 39.5¢ to 41¢/lb in March and ethylene producers asked for 3¢ to 4¢ more in April. Spot benzene was very high—in the $4/gal range in mid-April. PS producers say resin demand is improving, though current hikes are purely feedstock driven.

PET prices move up
PET prices rose 3¢/lb in March and 2¢ in April as suppliers were able to partially implement their 5¢ and 4¢ increases, respectively. A new 3¢/lb increase was announced for May 1 by all major players.

Contributing factors: Suppliers continue to aim for margin recovery and to regain some of the loss late last year of earlier resin price gains totaling 12¢ to 15¢/lb. Producers also hope to catch up with continued price increases in feedstocks, particularly paraxylene. They are trying to do this before the expected overcapacity situation arrives as new capacity expansions come on stream.