Clear containers
Clear containers with an integral handle have been an elusive goal, but recent adoption by a nationally recognized orange juice company has many wondering if their time has come.
Clear handled bottles got a kick start earlier this year when nationally recognized Simply Orange Juice Co., Apopka, Fla., an affiliate of the Minute Maid division of The Coca-Cola Co., decided to bottle its orange juice in extrusion blow molded 89-oz copolyester containers. Until now, clear containers with an integral handle have been an elusive goal. Some clear bottles have been stretch-blow molded and incorporated separate snap-on handles. And there has been limited success in extrusion blow molding containers of clarified PP and PVC. In those cases, the prime obstacles were the material’s lack of melt strength, brittleness, and inability to pass drop-impact tests.

Improved copolyester
Resin maker Eastman Chemical Co. and machine builder Bekum America Corp. teamed up more than three years ago to tackle this attractive high-growth market. The interest in clear handled containers was clearly evident at a recent Bekum open house and technical seminar attended by many food and beverage companies, bottlers, and blow molders. The first two clear handled applications—a 64-oz Indian River Select orange juice bottle in 2005 and a 48-oz POM Wonderful pomegranate juice container in 2006—were small-volume applications that validated the new copolyester developed by Eastman and Bekum’s extrusion blow technology. Now, the high-volume application at Simply Orange has many wondering if clear handled containers have arrived in force.

Simply Orange Juice Co.’s 89-oz container
Simply Orange Juice Co.’s 89-oz container uses a new Eastman copolyester and Bekum’s extrusion blow technology in the first high-volume, clear handleware application.

Some of the early success and optimism is attributed to Eastman’s Eastar EB062 copolyester, introduced in 2004. It is claimed to perform better than Eastman’s E-PET which was first offered to extrusion blow molders in the early 1990s. That material got poor reviews and gave extrusion blow molders a sour taste for polyesters in handleware. Eastman notes that EB062 is not PETG, but a branched amorphous copolyester. Its melt strength is twice that of PETG and similar to that of polycarbonate, Eastman says. It also boasts better toughness than other copolyesters and better drop impact as well. Its clarity and organoleptics (taste and odor) also beat those of PVC, according to Eastman.

The material has a processing temperature of 450 F. Maintaining that melt temperature is critical because excess heat can reduce melt strength. The material also sets up more quickly than HDPE and PVC, and shrinkage is less than that of HDPE. Eastman notes that bottle and mold design and process setup are important considerations in optimizing drop impact. In addition, proper drying is critical to avoid a reduction in the material’s inherent viscosity.

Bekum’s BM-406-D continuous-extrusion machine
Bekum’s BM-406-D continuous-extrusion machine features a special in-machine handleware deflasher and a simple linear cold-knife system that is unique in polyester bottle making.

Novel deflasher
On the machinery side, Bekum’s BM-406-D continuous-extrusion shuttle machine features a special in-machine deflasher for handleware. It acts like a peeling device and emulates a hand-trim operation. The peeling action results in less effect on the part and helps to maintain its drop-impact properties. The machine also features a simple linear cold-knife system, said to be unique in polyester bottle making, instead of the usual and more complicated hot knife.

The machine has two parisons per side, whose large diameter is said to aid processing and control of handled containers. A smooth-bore extruder of up to 120 mm diam. and 24:1 L/D is claimed to minimize shear heating and preserve melt strength. The machine also uses standard Bekum BKZ polyolefin extrusion heads and clamp force of 8 to 10 tons per cavity.

The Simply Orange containers have a 43-mm neck finish. At a recent Bekum demonstration, a four-cavity machine made 2-liter bottles in an 11-sec cycle at 1300 bottles/hr. Containers up to 10L can be made at 1000/hr. Both the Indian River and Simply Orange bottles are molded by CKS Packaging Inc., Atlanta. Other applications include organic milk, edible oil, and laundry care. Bekum and Eastman are also working on clear coextruded barrier handleware for similar applications.