New Starch-Based Bioplastics Arrive


By Matthew H. Naitove, Senior Editor

print this article Print This Article


Learn More

Read This Article...
Extruding Biopolymers: Packagin Reaps Cost Benefit of Going 'Green'

Higher Performing Biopolymers Seek New Market Opportunities

Online Exclusive: The Global Market for Biodegradable Polymer

Company Info

Cereplast, Inc.
Hawthorne, Calif.
(310) 676-5000

Clariant Masterbatches,
Holden, Mass.
(800) 782-7333

Colormatrix Corp.
Berea, Ohio
(216) 622-0100

DuPont Packaging & Industrial Polymers
Wilmington, Del.
(800) 438-7225

Plantic Technologies Ltd.,
Altona, Victoria, Australia
+61 (3) 9353 7900

PolyOne Corp.,
Avon Lake, Ohio
(440) 930-1000

Two new families of starch-based bioplastics are coming to the U.S. market. The one that’s available immedi-ately is an extension of the line of products supplied by Cereplast, Inc. This company has been offering 14 grades of compostable resins based on polylactic acid (PLA) or a thermoplastic starch mixed with some PLA. Now the firm is coming out with Cereplast Hybrid Resins, which are blends of plant starch with conventional polymers. These “hybrids” are not described as biodegradable, but rather as a way for manufacturers to reduce their reliance on oil and gas and increase their use of renewable resources. Because they are made with up to 50% conventional thermoplastics, Hybrids overcome what has been a limitation of most biobased resins to date—limited heat resistance in use and heat stability in processing.

PP/starch is very like PP
The first Cereplast Hybrid product on the market is Biopropylene CP Bio-PP-50. Chairman and CEO Frederic Scheer describes it as a patented mixture of polypropylene homopolymer with 50% starch and a blend of plasticizers or processing aids. Scheer says the product is made by reactive twin-screw compounding in which a chemical coupling occurs between the starch and PP matrix, which accounts for the material’s excellent properties.

Biopropylene has higher stiffness, strength, and heat resistance than un-filled PP but also has lower elongation and impact toughness. One notable advantage, says Scheer is Biopropylene’s easy printability, unlike standard PP. And unlike most biopolymers, it needs little or no drying.
The price of Biopropylene is similar to that of pure PP, though its 16% higher density will raise its cost in use somewhat. “We can offer long-term contracts at a guaranteed price,” notes Scheer. He will even consider toll compounding if the customer can get a better price for PP.

Targeting durables
Cereplast is aiming this product at durable goods rather than disposable packaging (though several food packagers reportedly are interested). Scheer says it has aroused considerable interest in the automotive field and is also targeted for housewares and other consumer products, toys, consumer electronics, cell-phone and computer housings, medical products, cosmetics packaging, CD/DVD cases, furniture, and building construction.

Biopropylene can be tailored for different uses. It can be formulated with any PP resin and various starches— corn, tapioca, wheat, and/or potato. Cereplast can vary the blend of starches for both properties and economics, Scheer said.

Biopropylene has been tested in sheet extrusion, thermoforming, blow molding, and injection molding, though not yet in blown film. It runs on conventional equipment in similar cycle times, but generally at lower temperatures. Processing requires low-shear screws and temperatures below 200 C (392 F). The resin is opaque and can be colored with standard PP masterbatches or colorants specifically designed for biopolymers by ?rms like PolyOne, Clariant, and Colormatrix.

Cereplast Biopropylene Vs. PP Homopolymer
Property CP-Bio-PP-50 Homo PP
Density, g/cc 1.04 0.9
Ult. Tens. Str., psi 2410 1650
Ultimate Elong., % 9.5

130.1

Flex. Modulus, psi 139,940

101,718

Tensile Mod., psi 299,280 119,480
Notched Izod Impact, ft-lb.in. 0.57 1.81
HDT@264 psi, F 142.3 129.9
MFI@190 C/2.16 kg.g/10 min 3 to 6 3

Though not intended to be compostable, Biopropylene is being tested for biodegradability and compostability. The starch component is expected to break down, leaving small fragments of PP. Scheer notes that the resin has already passed toxicity tests required for composting in the U.S. (ASTM D6400-04), Canada, and Western Europe. Cereplast is also seeking FDA approval for food contact.

Next year, Cereplast plans to launch Biopropylene grades with 60% and 70% starch, and after that will come Hybrids based on LDPE and HDPE.

Formable sheet & pellets
A second new family of starch-based materials—this one fully biodegradable and compostable—will be introduced in the ?rst half of next year by DuPont in collaboration with Plantic Technologies of Australia. Since 2003, Plantic has been making thermoformable sheets and injection moldable pellets of thermoplastic starch. Plantic uses high-amylose cornstarch that has been chemically modi?ed by hydroxy-propylation to make it behave as a thermoplastic. The starch is mixed with other polymeric and non-polymeric ingredi-ents, plasticizers and processing aids. One product is a wa-ter-soluble, sheet used for thermoformed candy trays. Other formulations have water resistance for up to 12 weeks.

Cereplast Biopropylene
Cereplast Biopropylene contains 50% chemically coupled starch in PP, which helps insulate buyers from swings in petrochemical prices

DuPont will market the formable sheet and molding pel-lets here under its own Biomax trade name. Initially they will be imported, though DuPont could produce the products itself in the future. DuPont will also explore uses of its modi?er ad-ditives in the starch resins, similar to what it has done with Biomax Strong tougheners for PLA.

Carol Casarino, DuPont’s technology manager for sus-tainable materials, says the formable sheet will have “value in use” competitive with OPS, APET, and PVC. She notes that the starch-based resins have the advantage of being inherently antistatic. DuPont is developing processing guidelines. Plantic’s datasheets indicate that melt temperatures should be below 200 C and some predrying is generally necessary.

According to Plantic, material densities range from 1.35 to 1.62. The formable sheet is fairly rigid (319 to 348 kpsi tensile modulus), but the molding pellets come in both rigid and ? exible grades (68 to 661 kpsi modulus). Tensile strength ranges from 913 to 6670 psi, elongation at break from 2% to 135%, Izod impact from 0.56 to 1.46 ft-lb/in., HDT at 66 psi from 92 to 117 F, and Vicat softening point from 104 to 158 F. The sheet has 60º gloss of 80 to 85 and transparency of 89% to 93%.