| New JL mixhead has a simplified, lower-pressure design, long nozzle to reach deep into cavities, and external micrometer adjustment (on top) for flow and pressure. |
The new JL (“jet-less”) family of L-shaped mixheads achieves good impingement mixing by means of speed and turbulence rather than pressure. This design eliminates the usual twin injectors for polyol and isocyanate. Instead, the two liquid components enter on opposite sides of a V-shaped feed chamber and then mix at high speed and turbulence inside a very narrow mixing chamber. The wider V-shaped feed opening requires lower initial pressure, but the flow accelerates and becomes more turbulent when it enters the tighter restriction of the narrow mixing chamber. Finally, the liquid stream enters a much longer and wider discharge duct, in which turbulence rapidly subsides into laminar flow, allowing the mix to be dispensed in a smooth stream without splashing, as with other L-shaped mixheads.
 |
 |
| No jets here: Chemicals enter V-shaped feed chamber at half the usual pressure. Flow accelerates and turbulence increases in the narrower mixing chamber. Turbulence subsides and laminar flow results in the large discharge duct. |
The V-shaped feed chamber is formed by the retraction of a central pin with a V-shaped front. At the end of the shot, it advances to clean out the feed chamber, while grooves on its sides allow the chemicals to recirculate.
A central needle inside the larger pin also advances at the end of the shot to clean out the mixing chamber. During the shot, the chemicals flow around the needle, which forms a variable restriction. Turning an external micrometer dial allows very fine manual adjustment of the front position of the needle, which varies the restriction and adapts it to the flow rate so as to maintain pressure in the V-shaped chamber. The needle can also be set automatically.
The discharge duct, at right angles to the mixing chamber, has its own cleaning rod, which is lubricated by a small amount of filtered and recirculated oil on each cycle. This main cleaning rod has a thicker end portion that wipes the inner surface of the duct. This wiping section of the rod is only 1 cm long; this small sliding surface reduces friction and reportedly solves problems of sticking in a long nozzle, especially with stickier formulations. The majority of the cleaning rod has a smaller diameter, reducing the weight of the head and making it easier handle manually.
SIMPLER, MORE EFFICIENT
Cannon says that computer simulations of the novel, patented design show it to be much more efficient than standard impingement mixing with jets. As a result, mixing pressure can be reduced from the usual 150 to 200 bar (2175 to 2900 psi) down to 70 to 80 bar (1015 to 1160 psi). This allows simplification of the whole metering circuit—pumps, filters, hoses, etc.—potentially reducing cost.
 |
 |
| JL head with central pin in recirculation position (left). Pin retracts (right) opening a V-shaped space for chemicals to enter, flowing around the central needle into the short, narrow mixing chamber and then into wide discharge duct (at a right angle). After the shot, the needle advances to clean the mixing chamber. |
In addition, a wider range of flow rates (5:1 ratio from minimum to maximum) can be handled by the same size mixing chamber. And the jet-less design does not require a skilled operator to adjust the jets for flow and pressure.
 |
Long discharge nozzle has cleaning rod with a short wiping section so as to avoid sticking. Rest of the rod shaft is thinner, making the head lighter and easier to handle. Rod is lubricated by recirculating oil (arrows at top) on each cycle. |
The internal geometry of this head is also said to allow better handling of foams with high-frothing blowing agents like HFCs and pentanes. The head can accommodate fillers, too.
Finally, the long nozzle on the head is designed to reach deep into complex molds for refrigeration or panels or pipe-in-pipe tooling.
FOR FOAMS & RIM
The first JL head on the market is the model JL 24/6, with 200-mm-long discharge duct having an internal diameter of 24 mm and mixing chamber of 6 mm diam. Total output range for this head is 300 to 2000 cc/sec. It has been tested for one year at up to 60,000 shots a month.
Cannon is aiming the first JL head initially at rigid foams. Later models will address flexible foams and RIM.