 RESIN GRADEb
¢/LB
¢/CU INc
 

 ABS

 

 
 
 MED IMPACT
  84 - 95  
  3.2 - 3.6  
 
 HI IMPACT
  89 - 125  
  3.3 - 4.7  
 
 X-HI IMPACT
  99 - 140  
  3.7 - 5.3  
 
 HI HEAT
  89 - 110  
  3.3 - 3.8  
 
 PIPE
  89 - 100  
  3.7 - 3.8  
 
 SHEET
  94 - 110  
  3.5 - 4.2  
 
 TRANSPARENT
  129 - 200  
  5.6 - 8.8  
 
 FITTINGS
  89 - 110  
  3.5 - 4.3  
 
 PLATING
  160  
  6.0  
 
 FLAME RET
  124 - 140  
  4.6 - 5.9  
 
 STRUCT FM
  87 - 97  
  3.2 - 4.3  
 
 10% GLASS
  129 - 140  
  4.8 - 5.6  
 
 30% GLASS
  124 - 136  
  4.6 - 6.3  
 
 ABS/PC ALLOY
  149 - 180  
  5.5 - 6.8  
 
 ABS/PVC ALLOY
  134 - 139  
  5.0 - 5.2  
 
 ABS/NYLON ALLOY
  194 - 350  
  9.0 - 16  
 


 ACETAL

 

 
 
 HOMOPOL
  151 - 172  
  7.7 - 8.7  
 
 20% GLASS
  171 - 235  
  8.7 - 11.9  
 
 COPOLYMER
  144 - 160  
  7.3 - 8.1  
 
 25% GLASS
  171 - 245  
  8.7 - 12.4  
 


 ACRYLIC

 

 
 
 G-P
  117  
  5.0  
 
 IMPACT
  192  
  8.2  
 


 ACRYLONITRILE COPOL

 

 
 
 EXTRUSION
  101 - 116  
  4.0 - 4.6  
 
 INJECTION
  120 - 135  
  4.8 - 5.4  
 


 ALKYD

65 - 74  

4.9 - 5.5  
 


 CELLULOSICS

 

 
 
 ACETATE
  187  
  8.6  
 
 CAB
  189  
  8.2  
 
 CAP
  189  
  8.2  
 


 DAP (G-P)

251 - 497  

16.7 - 34.7  
 


 EPOXY

 

 
 
 G-P RESIN
  116 - 126  
  NAd  
 
 COMPOUNDS
   
   
 
 C/B/Te
  123 - 166  
  9.4 - 12.9  
 
 R/C/Df
  208 - 271  
  15.3 - 20.1  
 
 SEMICONDUCTOR
   
   
 
 NOVOLAC
  193 - 228  
  13.1 - 15.9  
 
 ANHYDRIDE
  188 - 268  
  13.9 - 19.2  
 


 EVA

 

 
 
 INJECTION
  69 - 71  
  2.3 - 2.4  
 
 FILM EXTRU
  67 - 69  
  2.3  
 


 EVOH

330  

15  
 


 FLUORO-POLYMER

 

 
 
 CTFE
  5000 - 6000  
  385 - 462  
 
 ECTFE
  1200 - 1680  
  90.7 - 120  
 
 ETFE
  1205 - 1730  
  80.7 - 115.8  
 
 FEP
  971 - 1470  
  74.8 - 113.2  
 
 PFA
  1550 - 2520  
  120 - 195  
 
 PTFE
  500 - 950  
  33.5 - 63.6  
 
 PVDF
  693 - 1050  
  44.4 - 67.2  
 


 IONOMER

 

 
 
 PACKAGING
  127 - 166  
  4.3 - 6.0  
 
 INDUSTRIAL
  150 - 244  
  5.0 - 8.3  
 


 LIQUID-CRYSTAL POLYMERS

 

 
 
 INJECTION MIN FILLED
  690 - 1035  
  44.2 - 72.1  
 
 GLASS FILLED
  695 - 895  
  40 - 52  
 
 CARBON FILLED
  1700 - 2000  
  83.2 - 138.6  
 
 UNFILLED
  1000 - 1200  
  58 - 70  
 
 EXTRUSION UNFILLED
  1200 - 2200  
  60.5 - 110.9  
 


 MELAMINE COMPOUND

90 - 94  

5.5 - 5.6  
 


 MELAMINE/PHENOLIC COMPOUND

75 - 83  

4.5 - 5.0  
 


 NYLON

 

 
 
 TYPE 6
  139 - 159  
  5.7 - 6.5  
 
 MIN FILLED
  131 - 144  
  5.4 - 5.9  
 
 30% GLASS
  148 - 173  
  6.0 - 7.0  
 
 TYPE 66
  153 - 168  
  6.3 - 6.9  
 
 MIN FILLED
  151 - 159  
  6.2 - 6.5  
 
 30% GLASS
  142 - 192  
  5.8 - 7.9  
 
 TYPE 69
  250 - 276  
  9.7 - 10.7  
 
 TYPE 6/10
  286 - 313  
  12.4 - 13.6  
 
 TYPE 612
  400  
  15.3  
 
 30% GLASS
  309 - 311  
  14.7  
 
 40% GLASS
  309  
  14.7  
 
 TYPE 46
  295  
  12.6  
 
 TYPE 11
  329 - 341  
  13.6 - 14.1  
 
 30% GLASS
  331 - 350  
  15.0 - 15.8  
 
 40% GLASS
  347 - 360  
  17.7 - 18.5  
 
 TYPE 12
  318 - 341  
  12.1 - 13.0  
 
 30% GLASS
  327 - 350  
  14.7 - 15.8  
 
 50% GLASS
  299 - 340  
  15.6 - 17.8  
 
 TRANSPARENT AMORPHOUS
  247 - 360  
  10.3 - 15.0  
 


 PHENOLIC MOLD COMP

75  

3.8  
 
 REINFORCED GRADES
  105 - 268  
  6.1 - 16  
 


 POLYAMIDE-IMIDEg

 

 
 
 UNFILLED
  2750  
  148.5  
 
 30% GLASS
  2500  
  135  
 
 30% CARBON FIB.
  3500  
  185  
 


 POLYARYLATE

200 - 280  

8.8 - 12.3  
 


 POLYARYL SULFONE

440  

21.8  
 


 POLYBUTYLENE

 

 
 
 G-P
  94 - 96  
  3.1  
 
 FILM
  88 - 91  
  2.9  
 
 PIPE
   
   
 
 COLD WATER
  116 - 120  
  3.9 - 4.0  
 
 HOT WATER
  162 - 166  
  5.5 - 5.6  
 


 POLYCARBONATE

 

 
 
 INJECTION
  171 - 182  
  7.4 - 7.9  
 
 20% GLASS
  177 - 190  
  7.6 - 8.2  
 
 30% GLASS
  178 - 217  
  7.6 - 9.3  
 
 EXTRUSION
  145 - 180  
  6.3 - 7.8  
 
 BLOW MOLD
  150 - 185  
  7.0 - 7.5  
 
 STRUCT FOAM
  149 - 181  
  6.4 - 7.8  
 
 20% GLASS
  235 - 255  
  10.1 - 11.0  
 
 FR
  166 - 197  
  7.1 - 8.5  
 
 CD
  135 - 195  
  5.8 - 8.4  
 


 POLYESTER (TP) PBT TYPE

 

 
 
 UNFILLED
  145 - 150  
  6.8 - 7.3  
 
 HI-IMP
  165 - 175  
  7.8 - 8.3  
 
 30% GLASS, FR
  195 - 215  
  9.2 - 10.1  
 
 STRUCT FOAM
  159 - 165  
  NAd  
 


 PET

 

 
 
 BOTTLE (RAILCAR)
  78 - 80  
  4.0  
 
 MOD PET
   
   
 
 30% GLASS
  132 - 143  
  7.4  
 
 55% GLASS
  148 - 155  
  9.8  
 
 30% GLASS FLAME RET
  147 - 157  
  9.2  
 
 PETG COPOL
  114 - 124  
  5.2 - 5.6  
 
 RESIN GRADEb
¢/LB
¢/CU INc
 


 POLYESTER THERMOSET

 

 
 
 G-P ORTHO
  142 - 152  
  NAd  
 
 ISOPHTHALIC
  170 - 185  
  NAd  
 
 BIS-A
  205 - 225  
  NAd  
 


 PEEK

4400  

231  
 
 30% GLASS
  3300  
  173  
 


 POLYETHERIMIDE

641 - 646  

29.3 - 29.5  
 
 30% GLASS
  526 - 531  
  24.0 - 24.2  
 


 POLYETHERKETONE (PEK)

2950  

130.1  
 
 30% GLASS
  2600  
  153  
 


 POLYETHERSULFONE

350 - 400  

17.2 - 19.7  
 
 30% GLASS
  425 - 525  
  21 - 25.9  
 


 POLYETHYLENE (RAILCAR) LDPE

 

 
 
 G-P MOLDING & EXTRU
  81 - 83 Prices Went Up 
  2.6 - 2.7 Prices Went Up 
 
 INJECTION
  83 - 85 Prices Went Up 
  2.7 Prices Went Up 
 
 LID RESIN
  85 - 87 Prices Went Up 
  2.7 - 2.8 Prices Went Up 
 
 LINER
  80 - 82 Prices Went Up 
  2.6 Prices Went Up 
 
 CLARITY
  79 - 81 Prices Went Up 
  2.6 Prices Went Up 
 
 EXTRU COATG
  84 - 86 Prices Went Up 
  2.7 Prices Went Up 
 
 BLOW MOLD
  86 - 88 Prices Went Up 
  2.7 - 2.8 Prices Went Up 
 


 LLDPE, BUTENE BASED

 

 
 
 G-P MOLDING
  78 - 80 Prices Went Up 
  2.5 - 2.6 Prices Went Up 
 
 LME 30-DAYj
  80 - 85 Prices Went Up 
  2.6 Prices Went Up 
 
 FILM
  80 - 82 Prices Went Up 
  2.6 Prices Went Up 
 
 ROTOMOLD
  80 - 82 Prices Went Up 
  2.6 Prices Went Up 
 


 LLDPE, HAO-BASED

 

 
 
 G-P MOLDING
  81 - 83 Prices Went Up 
  2.6 Prices Went Up 
 
 LID RESIN
  91 - 93 Prices Went Up 
  2.9 Prices Went Up 
 
 LINER FILM
  84 - 86 Prices Went Up 
  2.7 Prices Went Up 
 


 HDPE

 

 
 
 G-P INJ MOLD
  78 - 80 Prices Went Up 
  2.6 Prices Went Up 
 
 FILM
  87 - 89 Prices Went Up 
  2.8 - 2.9 Prices Went Up 
 
 BLOW MOLD
  88 - 91 Prices Went Up 
  2.8 - 2.9 Prices Went Up 
 

 HMW-HDPE

 

 
 
 BLOW MOLDING
  85 - 87 Prices Went Up 
  2.7 - 2.8 Prices Went Up 
 
 FILM
  86 - 88 Prices Went Up 
  2.7 - 2.8 Prices Went Up 
 
 PIPE
  93 - 95 Prices Went Up 
  3.0 Prices Went Up 
 


 UHMW-PE

100 - 125  

3.6 - 3.7  
 


 PPE/PPO BASED RESIN

 

 
 
 INJECTION
  180  
  6.8  
 
 20% GLASSh
  283  
  12.3  
 
 30% GLASSh
  291  
  13.3  
 
 EXTRUSIONh
  242  
  9.2  
 
 STRUCT FM
  231  
  NAd  
 


 PPS

 

 
 
 40% GLASS
  450 - 520  
  27.0 - 31.2  
 
 55% GLASS/MINERAL
  345 - 420  
  22.7 - 27.7  
 
 65% GLASS/MINERAL
  270 - 315  
  18.9 - 22.1  
 


 POLYPROPYLENE (RAILCAR)

 

 
 
 G-P HOMOPOL INJECTION
  83 - 85 Prices Went Up 
  2.6 - 2.7 Prices Went Up 
 
 LME 30-DAYj
  68.4 Prices Went Up 
  2.2 Prices Went Up 
 
 EXTRUSION FIBER
  81 - 83 Prices Went Up 
  2.5 - 2.6 Prices Went Up 
 
 PROFILES
  86 - 88 Prices Went Up 
  2.7 - 2.8 Prices Went Up 
 
 RANDOM COPOL
   
   
 
 BLOW MOLDING
  87 - 89 Prices Went Up 
  2.8 Prices Went Up 
 
 FILM
  87 - 89 Prices Went Up 
  2.8 Prices Went Up 
 
 INJECTION
  86 - 88 Prices Went Up 
  2.7 - 2.8 Prices Went Up 
 
 IMPACT COPOL
   
   
 
 MED IMP
  97 - 99 Prices Went Up 
  3.1 - 3.2 Prices Went Up 
 
 HI IMP
  99 - 101 Prices Went Up 
  3.2 Prices Went Up 
 


 POLYSTYRENE (RAILCAR)

 

 
 
 G-P CRYSTAL
  88 - 94 Prices Went Up 
  3.3 - 3.5 Prices Went Up 
 
 HI HEAT
  91 - 97 Prices Went Up 
  3.4 - 3.6 Prices Went Up 
 
 HIPS
  89 - 94 Prices Went Up 
  3.3 - 3.5 Prices Went Up 
 
 SUPER HI IMP
  99 - 103 Prices Went Up 
  3.7 - 3.9 Prices Went Up 
 
 FR
  104 - 110 Prices Went Up 
  3.9 - 4.1 Prices Went Up 
 
 STRUCT FM (FR)
  105 - 108  
  NA  
 


 EPS

 

 
 
 UNMODIFIED
  85 - 88  
  NAd  
 
 MODIFIED
  86 - 90  
  NAd  
 


 POLYSULFONE

650 - 750  

29 - 33  
 
 10% GLASS 430 20.6
  799 - 875  
  36 - 39  
 
 30% GLASS 372 20.01
  699 - 775  
  31 - 35  
 


 POLYURETHANE (TP)

 

 
 
 ESTER TYPE
  185 - 255  
  8 - 11  
 
 ETHER TYPE
  245 - 295  
  10.6 - 13  
 


 PU ISOCYANATES

 

 
 
 POLYMERIC MDI
  125 - 145  
  NAd  
 
 80/20 TDI
  135 - 145  
  NAd  
 


 PVC RESIN (RAILCAR)

 

 
 
 G-P HOMOPOL
  58 - 60  
  NAd  
 
 PIPE
  57  
  NAd  
 
 FILM
  63 - 65  
  NAd  
 
 COPOLYMER FLOORING
  69 - 74  
  NAd  
 
 DISPERSION HOMOPOLY
  81 - 87  
  NAd  
 
 COPOLYMER
  86 - 90  
  NAd  
 
 CPVC PIPE COMPOUND
  119  
  NAd  
 


 PVDC

 

 
 
 EXTRUDABLE
  162  
  NAd  
 


 SILICONES

 

 
 
 MOLD. COMP.
  581 - 640  
  38.1 - 39.3  
 
 SPECIALTY GR.
  891 - 3148  
  NAd  
 
 SILICONE/EPOXY
  339 - 343  
  22.5 - 22.8  
 


 STYRENEACRYLIC

108 - 112  

3.7 - 4.0  
 


 SAN (G-P)

80 - 88  

3.0 - 3.3  
 


 STYRENE MALEIC ANHYDRIDE

 

 
 
 G-P
  110 - 115  
  4.2 - 4.3  
 
 HI IMP
  130 - 140  
  4.2 - 4.5  
 
 FR
  175 - 183  
  6.7 - 7.0  
 


 TP ELASTOMERS

 

 
 
 OLEFINIC
  70 - 76  
  2.4  
 
 POLYAMIDE
  300 - 350  
  10.9 - 12.7  
 
 POLYESTER
  200 - 310  
  8.8 - 13.6  
 
 STYRENIC
  82 - 237  
  2.9 - 8.3  
 


 UREA MOLDING COMPOUND

 

 
 
 BLACK & BROWN
   
   
 
 WHITE & IVORY
   
   
 


 VINYL ESTER

 

 
 
 COR RES
  218 - 235  
  NAd  
 
 HEAT & COR RES
  243 - 248  
  NAd  
 

 

PT Home | Zones | Suppliers | Materials Search | Machinery Search | Latest Issue | Article Search | Resin Prices | Blog | e-Newsletters |Subscribe | Advertise | Contact us

The Definitive Web Resource For Plastics Processors

© 2009 Gardner Publications, Inc