Greenerd Press & Machine will be showcasing the company’s hydraulic presses, which are capable of accommodating 40,000 tons with bed sizes exceeding 240" (6,100 mm).

Click Image to Enlarge

Greenerd Press & Machine will be showcasing the company’s hydraulic presses, which are capable of accommodating 40,000 tons with bed sizes exceeding 240" (6,100 mm). The presses are available in a variety of styles ranging from gap-frame and straight-side to die-spotting and forging. Custom presses can be designed for a range of manufacturing applications.