Stainless/Ceramic Sandwich Improves Pelletizer Die—January 2007


New "Anti-Freeze" die face for underwater pelletizers from Crown/CDL Technology Inc., Addison, Ill., has a 0.200-in. titanium carbide/stainless-steel surface layer braised onto 0.100 in. of pure zirconium ceramic, which is in turn braised onto the stainless-steel die body. The multi-material sandwich tolerates higher and lower temperatures than other die-plate materials, CDL says, allowing melt at up to 650 F to flow through the die holes and colder water down to 34 F to contact the cutting surface without polymer freeze-off. Also new is the Flex-Adjust automatic self-sharpening cycle, in which pneumatic pressure is applied by the rotating hub to the blades at intervals to sharpen the blades against the harder steel die surface. Tel: (630) 543-5240 . www.crown-cdl.com


 C.D.L. Technology
 511 Vista Ave.  Addison, IL 60101
 Phone (630) 543-5240 Fax (630) 543-4656

PT Home | Zones | Suppliers | Materials Search | Machinery Search | Latest Issue | Article Search | Resin Prices | Blog | e-Newsletters |Subscribe | Advertise | Contact us

The Definitive Web Resource For Plastics Processors

© 2009 Gardner Publications, Inc