Keeping-Up with Compounding

Reprocess Barrier Film Scrap into Sheet—February 2007


In tests late last year, a 0.75-in. single-screw lab extruder from Randcastle Extrusion Systems Inc., Cedar Grove, N.J., reprocessed five-layer PP/EVOH barrier film into 30-mil monolayer sheet, in which the EVOH was dispersed into sub-micron-size domains in the PP matrix. The 24:1 L/D screw used only two of Randcastle's Recirculator mixing sections to blend these incompatible materials, which would typically require more mixing sections and greater processing length. The customer intends to make two-layer coex sheet out of 60/40 PP and fivelayer barrier scrap. Tel: (973) 239-1150 . www.randcastle.com


 Randcastle Extrusion Systems
 220 Little Falls Road Unit 6  Cedar Grove, NJ 07009
 Phone (973) 239-1150 Fax (973) 239-0830

PT Home | Zones | Suppliers | Materials Search | Machinery Search | Latest Issue | Article Search | Resin Prices | Blog | e-Newsletters |Subscribe | Advertise | Contact us

The Definitive Web Resource For Plastics Processors

© 2009 Gardner Publications, Inc