PE Film Market Analysis: T-Shirt Bags
It's a huge business that will grow modestly over the next three years even in the face of environmental obstacles.
Last year, processors consumed about approximately 1.35 billion lb of polyethylene to produce grocery sacks, also known as t-shirt bags. Though ban, taxes and other environmental roadblocks are seemingly never-ending threat, the market should experience modest growth of 1.6% a year through 2017, when PE consumption for T-shirt bags will reach 1.420 billion lb.These are among the conclusions of the most recent study of the PE Film market conducted by Mastio & Co., St. Joseph, Mo.
Plastic bags still face competition from paper bags, as some consumers believe paper makes for a more natural and environmentally safe bag, says Mastio. Truth be told, paper manufacturing pollutes the water, releases dioxininto the atmosphere, contributes to acid rain, and depletes the tree population, the study points out.
Moreover, Mastio states, PE t-shirt bags consume 40% less energy than paper when produced, and generate 80% less solid waste than paper bags. Fewer atmospheric emissions are produced and less waterborne wastes are released with PE t-shirt bag production compared to paper bag production.
Currently, reusable cloth sacks continue to make inroads into this market due to the pressure from several state and city governments. Many states and cities are in the process or have already enacted legislation on single-use, paper and plastic bags that varies from an all-out ban to imposing a tax or bag fee on each bag at the point of sale. As a result, many stores are now selling their own reusable cloth or plastic sacks to consumers, Mastio point outs.
MATERIALS TRENDS
T-shirt bags are made primarily of HMW-HDPE and MMW-HDPE. HMW-HDPE is the resin of choice due to its superior strength in thinner gauges than LLDPE or LDPE. HDPE resins, particularly
UHMW-HDPE and HMW-HDPE grades, maintain the desired strength levels when downgauged, and have very high impact resistance.
LLDPE and LDPE resins are utilized when there is a desire for a strong bag that has improved printing properties, a softer texture, and more surface gloss. The various grades of LLDPE resin utilized included the following: LLDPE-butene, LLDPE-hexene and LLDPE-octene. LDPE-homopolymer resin was also incorporated in the production of t-shirt bags. The cost and appearance are typically higher for LLDPE bags when compared to HDPE bags, and some bag strength is sacrificed. With the small operating margins that most grocery stores experience, HDPE bags are a more feasible economic choice.
TECHNOLOGY TRENDS
T-shirt bags are made via the blown film process. Some 20 or so years ago, most t-shirt bags were single layer. Last year, according to the Mastio report, nearly 72% of t-shirt sacks produced were coextrusions, generally three layer. On average, says Mastio, PE t-shirt bags used 30% less material today than bags made five years ago. Advances in the PE resins used to produce t-shirt bags have reduced material requirements without decreasing bag strength.
MY TWO CENTS
Equipment builders argue that too many processors are making do with older equipment when newer technology will permit them to produce better quality films at higher speeds. One industry source estimates that more than 70% of the 20 billion lb/yr of blown film is currently processed on equipment that’s 10 years old or older. But T-shirt bagmaking is a highly competitive market will razor-thin margins, making big capital equipment investments a big challenging.
That argument aside, if more processors followed the lead of Novolex (Hilex Poly), staving off environmental threats might be a bit less challenging. The firm made a huge commitment in setting up an infrastructure allowing to collect post-consumer film and reprocess it into new bags. Read that story here.
Related Content
Troubleshooting Screw and Barrel Wear in Extrusion
Extruder screws and barrels will wear over time. If you are seeing a reduction in specific rate and higher discharge temperatures, wear is the likely culprit.
Read MoreExtruder Alignment: Important, but Only Half the Equation
The other half? Aligning and supporting downstream equipment. Here are best practices.
Read MoreSpecialty Purging Compounds Optimize Color and Material Changeovers
Selecting of the correct purging compound can speed up material and color changeover time and reduce scrap. You’ll even save on material.
Read MoreAvoid Four Common Traps In Granulation
Today, more than ever, granulation is an important step in the total production process. Our expert explains a few of the many common traps to avoid when thinking about granulators
Read MoreRead Next
Advanced Recycling: Beyond Pyrolysis
Consumer-product brand owners increasingly see advanced chemical recycling as a necessary complement to mechanical recycling if they are to meet ambitious goals for a circular economy in the next decade. Dozens of technology providers are developing new technologies to overcome the limitations of existing pyrolysis methods and to commercialize various alternative approaches to chemical recycling of plastics.
Read MoreWhy (and What) You Need to Dry
Other than polyolefins, almost every other polymer exhibits some level of polarity and therefore can absorb a certain amount of moisture from the atmosphere. Here’s a look at some of these materials, and what needs to be done to dry them.
Read MoreProcessor Turns to AI to Help Keep Machines Humming
At captive processor McConkey, a new generation of artificial intelligence models, highlighted by ChatGPT, is helping it wade through the shortage of skilled labor and keep its production lines churning out good parts.
Read More