SUNTEST XXL/XXL+

Our largest and only freestanding SUNTEST flatbed instrument.

Our largest and only freestanding SUNTEST flatbed instrument. The 3081 cm2 specimen tray is perfect for high volume testing and testing of large components and three-dimensional parts. · Total exposure area: 3081 cm² · Easy-to-use touch screen panel and ergonomic tilting to maximize comfort during operation · Controlled temperature (BST/BPT or CHT or both simultaneously) · Temperature range: BST 30 °C to 100 °C CHT up to 70°C · Controlled irradiance (300-400 nm or 340 nm or 420 nm) – easy switch from one control range to another (no hardware change needed) · Control of relative humidity (up to 95%) and spray cycles · Measurement and control of Chamber Air Temperature (CHT) (max. 70°C during light phase) · 3 air-cooled xenon lamps with adjustable power range between 1.7 and 2.1 kW · Specimen tray with 5° slope (as recommended in many standards) for optimum spray water drain · Software language selectable between German, English and French