Solving the Mystery of Melt Temperature

Two new types of sensors are said to be the first practical means to measure "true" melt temperature inside the machine or mold.

Share

However much we think we know about the injection molding process today, I’ve been talking lately with a number of molders and molding experts, who agree that we still don’t know very much about what is happening to melt temperature inside the machine and mold. Some of them call it, frankly, a “mystery.”

 

I’m no Sherlock Holmes, but I deduce that a solution—or two—may have arrived. Keep an eye out for our October issue, which should appear online next week and in the mail soon after.

 

Up to now, molders have had two options. They could put a thermocouple in the nozzle, but its readings are affected by the surrounding steel as much as the melt. And if the sensor projects into the melt stream, away from the steel, it is subject to wear and damage, and induces extra shearing that distorts the reading.

 

I’m told the only practical means of measuring melt temperature is to purge a blob of melt and shove a sensor into it by hand—a procedure that is both clumsy and plagued by numerous variables and inconsistencies, not to mention that it interrupts actual molding.

 

Enter Md Plastics in Youngstown, Ohio, which is offering a unique melt-temperature sensor that can be placed in the machine nozzle, mold cavity, or mold vent. As explained by company president Mike Durina, the sensor responds to both temperature and pressure, which makes its operation a little complicated to explain, so I recommend reading the full Close Up article. In short, during the injection filling and packing stages, the sensor reading reflects the total energy input (or “work”) into the melt. However, at the end of the cooling stage, before screw recovery starts, when the melt is under little pressure, the sensor reading stabilizes at a level that corresponds to melt temperature alone.

 

The manager of one molder’s tech center got his best technicians together and had them all perform manual-purge temperature measurements, and the average of their results corresponded nicely with the readings of Md Plastics’ Temp-Tek sensor. “Pretty darn good,” he concluded.

 

Durina notes that the Temp-Tek sensor can also be used in other processes: In blow molding, it could be placed in the mold or inside the parison to measure the air temperature there. In extrusion, it could be placed in the melt stream or in the die; it could also measure the air temperature inside a blown film bubble, providing information not usually available. I thermoforming, the sensor could be mounted between the sheet and the mold.

 

While I was researching the story on that sensor, I learned that Futaba Corp. of America, Schaumburg, Ill., is introducing to the U.S. a reportedly unique infrared sensor (photo) that directly senses the temperature of the melt without being influenced by the surrounding steel. It’s fast—8 millisec response time—and provides a wealth of information: For example, if placed in a mold cavity, the measured cooling rate correlates with the degree of packing of that part. It’s being used in Japan by major customers such as Toyota, Nissan, Panasonic, and Denso. There’s more on this in the October Keeping Up section. By the way, the person to contact at Futaba is Mr. Yasuo Ishiwata (yishiwata@futaba.com).

Vecoplan
Advantage temperature control units
Create custom Smartflow assemblies on-line, 24/7.
New Tinius Olsen VectorExtensometer testing
Insert molding automation
Konica Minolta CM-36dG
Vacuum conveying powders to extruders compounding
Dover Clear
Guill - World Leader in Extrusion Tooling
Blending Revolution
Dri-Air
Cranes, Conveyors, Racks, Loaders, Accessories

Related Content

SPONSORED

Fully Automated Extrusion Process Enables Use of Composites for Manufacturing Pressure Tanks

Amtrol was looking for a more cost-effective means to produce thin-wall liners for a new line of pressure tanks. With the help of a team of suppliers, they built one of the world’s most sophisticated extrusion lines.

Read More
SPONSORED

Specialty Purging Compounds Optimize Color and Material Changeovers

Selecting of the correct purging compound can speed up material and color changeover time and reduce scrap. You’ll even save on material.

Read More

How Polymer Melts in Single-Screw Extruders

Understanding how polymer melts in a single-screw extruder could help you optimize your screw design to eliminate defect-causing solid polymer fragments.  

Read More
Film Extrusion

Formulating LLDPE/LDPE Blends For Abuse–Resistant Blown Film

A new study shows how the type and amount of LDPE in blends with LLDPE affect the processing and strength/toughness properties of blown film. Data are shown for both LDPE-rich and LLDPE-rich blends.

Read More

Read Next

monitoring

New Sensor Tech Monitors State of the Melt During Molding

Detect ‘true’ melt temperature, viscosity variations, melt density, and much more, throughout the molding cycle.

Read More
Extrusion

Understanding Melting in Single-Screw Extruders

You can better visualize the melting process by “flipping” the observation point so that the barrel appears to be turning clockwise around a stationary screw.

Read More
mold, mould track, digital tracking, molding