PT Online

 

Resin Pricing–September 2010


[ Analyses | Recycled Resin Prices ]


Market Prices Effective Mid-September A


 RESIN GRADEb ¢/LB ¢/CU INc
Redeye OnDemand


 ABS

 

 
 
 MED IMPACT
  95 - 115  
  3.6 - 4.4  
 
 HI IMPACT
  100 - 135  
  3.7 - 5.1  
 
 X-HI IMPACT
  15 - 155  
  4.3 - 5.8  
 
 HI HEAT
  95 - 130  
  3.6 - 5.0  
 
 PIPE
  90 - 100  
  3.3 - 3.7  
 
 SHEET
  95 - 110  
  3.8 - 4.4  
 
 TRANSPARENT
  139 - 210  
  5.4 - 8.2  
 
 FITTINGS
  99 - 120  
  3.7 - 8.0  
 
 PLATING
  170  
  6.4  
 
 FLAME RET
  125 - 145  
  5.4 - 6.2  
 
 STRUCT FM
  97 - 107  
  4.3 - 4.7  
 
 10% GLASS
  139 - 150  
  5.3 - 5.7  
 
 30% GLASS
  134 - 146  
  5.0 - 5.5  
 
 ABS/PC ALLOY
  159 - 190  
  6.0 - 7.2  
 
 ABS/PVC ALLOY
  144 - 149  
  5.4 - 5.6  
 
 ABS/NYLON ALLOY
  204 - 360  
  7.7 - 13.6  
 

 ACETAL

 

 
 
 HOMOPOL
  151 - 172  
  7.7 - 8.7  
 
 20% GLASS
  171 - 235  
  8.7 - 11.9  
 
 COPOLYMER
  144 - 160  
  7.3 - 8.1  
 
 25% GLASS
  171 - 245  
  8.7 - 12.4  
 

 ACRYLIC

 

 
 
 G-P
  117  
  5.0  
 
 IMPACT
  192  
  8.2  
 

 ACRYLONITRILE COPOL

 

 
 
 EXTRUSION
  101 - 116  
  4.0 - 4.6  
 
 INJECTION
  120 - 135  
  4.8 - 5.4  
 

 ALKYD

65 - 74  

4.9 - 5.5  
 

 CELLULOSICS

 

 
 
 ACETATE
  187  
  8.6  
 
 CAB
  189  
  8.2  
 
 CAP
  189  
  8.2  
 

 DAP (G-P)

251 - 497  

16.7 - 34.7  
 

 EPOXY

 

 
 
 G-P RESIN
  116 - 126  
  NAd  
 
 COMPOUNDS
   
   
 
 C/B/Te
  123 - 166  
  9.4 - 12.9  
 
 R/C/Df
  208 - 271  
  15.3 - 20.1  
 
 SEMICONDUCTOR
   
   
 
 NOVOLAC
  193 - 228  
  13.1 - 15.9  
 
 ANHYDRIDE
  188 - 268  
  13.9 - 19.2  
 

 EVA

 

 
 
 INJECTION
  69 - 71  
  2.3 - 2.4  
 
 FILM EXTRU
  67 - 69  
  2.3  
 

 EVOH

330  

15  
 

 FLUORO-POLYMER

 

 
 
 CTFE
  5000 - 6000  
  385 - 462  
 
 ECTFE
  1200 - 1680  
  90.7 - 120  
 
 ETFE
  1205 - 1730  
  80.7 - 115.8  
 
 FEP
  971 - 1470  
  74.8 - 113.2  
 
 PFA
  1550 - 2520  
  120 - 195  
 
 PTFE
  500 - 950  
  33.5 - 63.6  
 
 PVDF
  750 - 1200  
  48 - 76.9  
 

 IONOMER

 

 
 
 PACKAGING
  127 - 166  
  4.3 - 6.0  
 
 INDUSTRIAL
  150 - 244  
  5.0 - 8.3  
 

 LIQUID-CRYSTAL POLYMERS

 

 
 
 INJECTION MIN FILLED
  690 - 1035  
  44.2 - 72.1  
 
 GLASS FILLED
  695 - 895  
  40 - 52  
 
 CARBON FILLED
  1700 - 2000  
  83.2 - 138.6  
 
 UNFILLED
  1000 - 1200  
  58 - 70  
 
 EXTRUSION UNFILLED
  1200 - 2200  
  60.5 - 110.9  
 

 MELAMINE COMPOUND

90 - 94  

5.5 - 5.6  
 

 MELAMINE/PHENOLIC COMPOUND

75 - 83  

4.5 - 5.0  
 

 NYLON

 

 
 
 TYPE 6
  134 - 169  
  5.5 - 6.9  
 
 MIN FILLED
  126 - 154  
  6.2 - 8.2  
 
 30% GLASS
  148 - 173  
  6.0 - 7.0  
 
 TYPE 66
  153 - 168  
  6.3 - 6.9  
 
 MIN FILLED
  151 - 159  
  6.2 - 6.5  
 
 30% GLASS
  142 - 192  
  5.8 - 7.9  
 
 TYPE 69
  250 - 276  
  9.7 - 10.7  
 
 TYPE 6/10
  286 - 313  
  12.4 - 13.6  
 
 TYPE 612
  400  
  15.3  
 
 30% GLASS
  309 - 311  
  14.7  
 
 40% GLASS
  309  
  14.7  
 
 TYPE 46
  295  
  12.6  
 
 TYPE 11
  650 - 750  
  24.3 - 28  
 
 30% GLASS
  NAd - NAd  
  NAd - NAd  
 
 40% GLASS
  NAd - NAd  
  NAd - NAd  
 
 TYPE 12
  318 - 341  
  12.1 - 13.0  
 
 30% GLASS
  327 - 350  
  14.7 - 15.8  
 
 50% GLASS
  299 - 340  
  15.6 - 17.8  
 
 TRANSPARENT AMORPHOUS
  247 - 360  
  10.3 - 15.0  
 

 PHENOLIC MOLD COMP

75  

3.8  
 
 REINFORCED GRADES
  105 - 268  
  6.1 - 16  
 

 POLYAMIDE-IMIDEg

 

 
 
 UNFILLED
  2750  
  148.5  
 
 30% GLASS
  2500  
  135  
 
 30% CARBON FIB.
  3500  
  185  
 

 POLYARYLATE

200 - 280  

8.8 - 12.3  
 

 POLYARYL SULFONE

440  

21.8  
 

 POLYBUTYLENE

 

 
 
 G-P
  94 - 96  
  3.1  
 
 FILM
  88 - 91  
  2.9  
 
 PIPE
   
   
 
 COLD WATER
  116 - 120  
  3.9 - 4.0  
 
 HOT WATER
  162 - 166  
  5.5 - 5.6  
 

 POLYCARBONATE

 

 
 
 INJECTION
  163 - 178  
  7.0 - 7.7  
 
 20% GLASS
  169 - 186  
  8.2 - 9.0  
 
 30% GLASS
  170 - 212  
  8.8 - 10.3  
 
 EXTRUSION
  138 - 176  
  6.0 - 7.6  
 
 BLOW MOLD
  143 - 181  
  6.2 - 7.8  
 
 STRUCT FOAM
  142 - 177  
  6.2 - 7.7  
 
 20% GLASS
  224 - 248  
  9.8 - 10.8  
 
 FR
  158 - 193  
  6.9 - 8.4  
 
 CD
  129 - 191  
  5.6 - 8.3  
 

 POLYESTER (TP) PBT TYPE

 

 
 
 UNFILLED
  145 - 150  
  6.8 - 7.3  
 
 HI-IMP
  165 - 175  
  7.8 - 8.3  
 
 30% GLASS, FR
  195 - 215  
  9.2 - 10.1  
 
 STRUCT FOAM
  159 - 165  
  NAd  
 

 PET

 

 
 
 BOTTLE (RAILCAR)
  73 - 76 Prices Went Up 
  3.7 - 3.8  
 
 MOD PET
   
   
 
 30% GLASS
  132 - 143  
  7.4  
 
 55% GLASS
  148 - 155  
  9.8  
 
 30% GLASS FLAME RET
  147 - 157  
  9.2  
 
 PETG COPOL
  114 - 124  
  5.2 - 5.6  
 

 POLYESTER THERMOSET

 

 
 
 G-P ORTHO
  155 - 166 Prices Went Up 
  NAd  
 
 ISOPHTHALIC
  179 - 200 Prices Went Up 
  NAd  
 
 BIS-A
  214 - 239 Prices Went Up 
  NAd  
 

 PEEK

4400  

231  
 
 30% GLASS
  3300  
  173  
 

 POLYETHERIMIDE

641 - 646  

29.3 - 29.5  
 
 30% GLASS
  526 - 531  
  24.0 - 24.2  
 

 POLYETHERKETONE (PEK)

2950  

130.1  
 
 30% GLASS
  2600  
  153  
 

 POLYETHERSULFONE

350 - 400  

17.2 - 19.7  
 
 30% GLASS
  425 - 525  
  21 - 25.9  
 

 POLYETHYLENE (RAILCAR) LDPE

 

 
 
 G-P MOLDING & EXTRU
  78 - 80  
  2.6  
 
 INJECTION
  80 - 82  
  2.6 - 2.7  
 
 LID RESIN
  81 - 83  
  2.7  
 
 LINER
  76 - 78  
  2.5 - 2.6  
 
 CLARITY
  74 - 76  
  2.5  
 
 EXTRU COATG
  81 - 83  
  2.7  
 
 BLOW MOLD
  83 - 85  
  2.7 - 2.8  
 

 LLDPE, BUTENE BASED

 

 
 
 G-P MOLDING
  68 - 70  
  2.4  
 
 LME 30-DAYj
  47.4 Prices Went Up 
  1.8  
 
 FILM
  70 - 72  
  2.4  
 
 ROTOMOLD
  70 - 72  
  2.4  
 

 LLDPE, HAO-BASED

 

 
 
 G-P MOLDING
  72 - 74  
  2.4 - 2.5  
 
 LID RESIN
  83 - 85  
  2.7 - 2.8  
 
 LINER FILM
  76 - 78  
  2.5 - 2.6  
 

 HDPE

 

 
 
 G-P INJ MOLD
  69 - 71  
  2.4  
 
 FILM
  78 - 80  
  2.6 - 2.7  
 
 BLOW MOLD
  72 - 74  
  2.4 - 2.5  
 

 HMW-HDPE

 

 
 
 BLOW MOLDING
  76 - 78  
  2.6  
 
 FILM
  77 - 79  
  2.6  
 
 PIPE
  88 - 90  
  2.8 - 2.9  
 

 UHMW-PE

1.22 - 1.52  

4.1 - 5.1  
 

 PPE/PPO BASED RESIN

 

 
 
 INJECTION
  180  
  6.8  
 
 20% GLASSh
  283  
  12.3  
 
 30% GLASSh
  291  
  13.3  
 
 EXTRUSIONh
  242  
  9.2  
 
 STRUCT FM
  231  
  NAd  
 

 PPS

 

 
 
 40% GLASS
  450 - 520  
  27.0 - 31.2  
 
 55% GLASS/MINERAL
  345 - 420  
  22.7 - 27.7  
 
 65% GLASS/MINERAL
  270 - 315  
  18.9 - 22.1  
 

 POLYPROPYLENE (RAILCAR)

 

 
 
 G-P HOMOPOL INJECTION
  81 - 83 Prices Went Up 
  2.6  
 
 LME 30-DAYj
  49.6 Prices Went Up 
  1.6  
 
 EXTRUSION FIBER
  79 - 81 Prices Went Up 
  2.6 - 2.6  
 
 PROFILES
  85 - 82 Prices Went Up 
  2.7  
 
 RANDOM COPOL
   
   
 
 BLOW MOLDING
  85 - 87 Prices Went Up 
  2.7  
 
 FILM
  86 - 88 Prices Went Up 
  2.7 - 2.8  
 
 INJECTION
  88 - 91 Prices Went Up 
  2.8  
 
 IMPACT COPOL
   
   
 
 MED IMP
  96 - 98 Prices Went Up 
  3.1 - 3.2  
 
 HI IMP
  98 - 100 Prices Went Up 
  3.2  
 

 POLYSTYRENE (RAILCAR)

 

 
 
 G-P CRYSTAL
  61 - 67 Prices Went Down
  2.3 - 2.5  
 
 HI HEAT
  64 - 69 Prices Went Down
  2.4 - 2.6  
 
 HIPS
  70 - 76 Prices Went Down
  2.6 - 2.8  
 
 SUPER HI IMP
  77 - 84 Prices Went Down
  2.9 - 3.1  
 
 FR
  80 - 85 Prices Went Down
  3.0 - 3.2  
 
 STRUCT FM (FR)
  66 - 68  
  2.5  
 

 EPS

 

 
 
 UNMODIFIED
  89 - 92  
   
 
 MODIFIED
  90 - 94  
  NAd  
 

 POLYSULFONE

650 - 750  

29 - 33  
 
 10% GLASS 430 20.6
  799 - 875  
  36 - 39  
 
 30% GLASS 372 20.01
  699 - 775  
  31 - 35  
 

 POLYURETHANE (TP)

 

 
 
 ESTER TYPE
  185 - 255  
  8 - 11  
 
 ETHER TYPE
  245 - 295  
  10.6 - 13  
 

 PU ISOCYANATES

 

 
 
 POLYMERIC MDI
  125 - 145  
  NAd  
 
 80/20 TDI
  135 - 145  
  NAd  
 

 PVC RESIN (RAILCAR)

 

 
 
 G-P HOMOPOL
  50 - 51 Prices Went Up 
  NAd  
 
 PIPE
  47  
  NAd  
 
 FILM
  55 Prices Went Up 
  NAd  
 
 COPOLYMER FLOORING
  71 - 74  
  NAd  
 
 DISPERSION HOMOPOLY
  81 - 87  
  NAd  
 
 COPOLYMER
  86 - 90  
  NAd  
 
 CPVC PIPE COMPOUND
  119  
  NAd  
 

 PVDC

 

 
 
 EXTRUDABLE
  162  
  NAd  
 

 SILICONES

 

 
 
 MOLD. COMP.
  581 - 640  
  38.1 - 39.3  
 
 SPECIALTY GR.
  891 - 3148  
  NAd  
 
 SILICONE/EPOXY
  339 - 343  
  22.5 - 22.8  
 

 STYRENEACRYLIC

108 - 112  

3.7 - 4.0  
 

 SAN (G-P)

80 - 88  

3.0 - 3.3  
 

 STYRENE MALEIC ANHYDRIDE

 

 
 
 G-P
  110 - 115  
  4.2 - 4.3  
 
 HI IMP
  130 - 140  
  4.2 - 4.5  
 
 FR
  175 - 183  
  6.7 - 7.0  
 

 TP ELASTOMERS

 

 
 
 OLEFINIC
  70 - 76  
  2.4  
 
 POLYAMIDE
  300 - 350  
  10.9 - 12.7  
 
 POLYESTER
  200 - 310  
  8.8 - 13.6  
 
 STYRENIC
  82 - 237  
  2.9 - 8.3  
 

 UREA MOLDING COMPOUND

 

 
 
 BLACK & BROWN
   
   
 
 WHITE & IVORY
   
   
 

 VINYL ESTER

 

 
 
 COR RES
  225 - 249 Prices Went Up 
  NAd  
 
 HEAT & COR RES
  250 - 262 Prices Went Up 
  NAd  
 

KEY: Colored areas indicate pricing activity. An arrow () indicates direction of price change. aTruckload, unless otherwise specified. bUnfilled, natural color, unless otherwise specified. cBased on typical or average density. dNot applicable. eNovolac and anhydride grades for coils, bushings, transformers. fNovolac and anhydride grades for resisitors, capacitors, diodes. gIn quantities of 20,000 lb. h19,800-lb load. jLME 30-day futures contract for lots of 54,564 lb..

PT Home | Zones | Suppliers | Materials | Machinery | Articles | Resin Prices | News | Subscribe