Airflow 150-250 cfm

Metal silos are affected by the weather conditions surrounding them. They can become damp internally from sweat on their sidewalls caused by changes in humidity and temperature. This moisture can be transferred to the material stored in the silo.

Silo dehumidifiers are not intended to dry the material stored inside the silo. Instead, they operate on the simple principle of providing a blanket of dry air in the space above the material to keep the material from picking up additional moisture while in storage.

Silo dehumidifiers are usually installed in the base of a silo and one dehumidifier may serve more than one silo.