oz in in in in in
NT 440 14 - 130 26.6 56.1 9.8 46.3x45.3 33.07x33.07
NT 550 30 - 130 36.6 67.7 9.8 50.8x50.8 36.22x36.22
NT 750 72 - 195 39.4 78.7 15.8 57.1x60.0 40.16x40.16
NT 935 72 - 195 47.2 94.5 17.7 68.3x60.8 49.21x39.37
NT 1125 72 - 195 51.9 103.9 15.7 81.5x70.9 61.00x47.20

 

 

Metric

Powerline Model/Tonnage Injection Size Range Clamp
Stroke
Max
Daylight
Min. Mold Thickness Platen
Size
Tie Rod Clearance
gm mm mm mm mm mm
NT 440 397-3686 675 1425 250 1175x1150 840x840
NT 550 850-3686 880 1720 250 1290x1290 920x920
NT 750 2041-5528 1000 2000 400 1450x1520 1020x1020
NT 935 2041-5528 1200 2400 450 1735x1545 1250x1000
NT 1125 2041-5528 1320 2640 400 2070x1800 1550x1200