Home
»
Systems
» Rolls and Cut Sheet
Rolls and Cut Sheet
Whether producing mono- or multi-layer sheet, many sheet extrusion systems produce rolls of finished sheet, or stacks of sheet that has been cut-to-length.
These "off-line" systems are used by companies who make frequent color or tooling changes, produce smaller volume parts, or when narrow (under 30" width) thermoformers are used. Finished rolls or stacks of cut sheet are also run by firms who extrude sheet to be used as sheeting, and by custom sheet producers.
A variety of fully automated winders are available, including jumbo roll, turret, and fixed shaft styles.
Sheet can also be cut-to-length by precision fully automated cut-off devices, in which case specialized hump conveyors, run off tables and stackers may be supplied.
WORLD STANDARD SHEET EXTRUSION SYSTEM
900 Lb/Hr (400 Kg/Hr) - PS/PET
750 Lb/Hr (340 Kg/Hr) - PP
WORLD STANDARD SHEET EXTRUSION SYSTEM
3200 Lb/Hr (1450Kg/Hr) - PS / PET
2400 Lb/Hr (1100 Kg/Hr) - PP
900 Lb/Hr (400 Kg/Hr) - PS/PET
750 Lb/Hr (340 Kg/Hr) - PP
3-1/2" (90 mm) 32/1 L/D Main Extruder
- Rigid steel machine framework
- AC drive system
- Heavy duty gear reducer
- Bimetallic lined barrel with heater / coolers installed
- Extrusion screw designed for the specific polymer
- Extruder Tooling
• Screen changer
• Melt pump
• Static mixer
• Adapter kit and heaters as required
Sheet Die
- Sheet die with manifold designed for the application
- Support assembly
Sheet Take-off
- Pneumatic roll actuation
- Chain drive arrangement
- Individual roll drives - optional
- Coating and gauging equipment as needed or requested
- Heat exchange system located under conveyor
- Pull roll station with edge trim slitters
- Winding system to suit application or power shear for cut-to-length sheet
System Electrical and Control
- Designed to handle all major power supplies
- Color touch screen HMI
- PLC control and coordination of all heat zones and drive motors
- High end control features available as requested
3200 Lb/Hr (1450Kg/Hr) - PS/PET
2400 Lb/Hr (1100 Kg/Hr) - PP
6" (150 mm) 32/1 L/D Main Extruder
- Rigid steel machine framework
- AC drive system
- Heavy duty gear reducer
- Bimetallic lined barrel with heater / coolers installed
- Extrusion screw designed for the specific polymer
- Extruder Tooling
• Screen changer
• Melt pump
• Static mixer
• Adapter kit and heaters as required
Sheet Die
- Sheet die with manifold designed for the application
- Support assembly
Sheet Take-off
- Three roll primary cooling and polishing stack
- Pneumatic roll actuation
- Chain drive arrangement
- Individual roll drive - optional
- Coating and gauging equipment as needed or requested
- Heat exchange system located under conveyor
- Pull rolls station with edge trim slitters
- Winding system or power shear for cut-to-length sheet
System Electrical and Control
- Designed to handle all major power supplies
- Color touch screen HMI
- PLC control and coordination of all heat zones and drive motors
- High end control features available as requested