Recap of Refocus Sustainability & Recycling Summit
Sustainable materials must meet or exceed the performance of their traditional competitors; could ocean plastic be coming to cars; and more.
The Plastics Industry Association (PLASTICS) held the second annual Refocus Sustainability & Recycling Summit with the sustainability division of SPE (Society of Plastics Engineers) as the principal programming partner, in Orlando, Fla., June 27-29 (next year Refocus will take place during NPE2018). The summit is designed for the plastics industry and covered a variety of topics and challenges facing the sector when it comes to expanding the use of recycled plastics and driving sustainability in manufacturing. Here are some of the highlights from the event:
Sustainable Materials for Ford Vehicles
The summit kicked off with a presentation from Debbie Mielewski, senior technical leader of sustainable and emerging materials for Ford Motor Co. Mielewski detailed the opportunities and challenges in working with sustainable materials (photo courtesy PLASTICS).
“Materials that are greener have to be just as good or better as petroleum—there must be no comprise because of using ‘green’,” she said. “Sustainable materials can be economically viable when you use it in high volume.”
Some of the projects Mielewski and her team have worked on include the implementation of soy foam on the 2008 Mustang and producing a fiber that was used in a seat fabric made from a hybrid blend of 100% recycled materials, including post-industrial fiber and post-consumer water bottles. In addition, Ford has produced bio-composites based on PP and PA6-reinforced with recycled carbon fiber and cellulose fibers for the fabrication of injection molding automotive parts.
Projects in the pipeline include research and development propositions at the material design level and circular economy solutions including potentially making car parts from recycled ocean plastics.
“With ocean plastic, we are starting a project with interns getting mixed plastic material from ocean and trying to figure out what to do with it,” she said. “Is it degraded too much to use it? We’ll report on that next time.”
Circular Economy and New Plastics Economy
There was a lot of discussion about the circular economy. One key presentation came from Susan Graff, vice president and partner of Resource Recycling Systems. She said that the drive for efficiency has produced innovative lightweight formats. However, efficiency gains are not enough and sustainability and the circular economy should be about using less new plastic.
So how can a company work toward a circular economy vision?
She recommends setting ambitious, public commitments for source reduction, waste avoidance and use of recycled feedstock. She said companies should support sustainable material management and use of recycling best practices where they operate, and she stated that everyone in the value chain has a role to play to improve recycling.
99% Bio-Content PE foam
Sealed Air discussed its renewable bio-content PE foam—a new patent-pending technology. The company says it’s the first to introduce a renewable 99% bio-content PE foam that was made at commercially viable extrusion rates. Sealed Air worked with Braskem on the bio-sourced PE resin. It features renewable feedstock such as sugarcane based ethanol and other renewable resource materials. The renewable PE foam’s output rate is reportedly same as petroleum-based PE foam.
Global Sustainability Initiatives
Sandeep Kulkarni, senior principal scientist global beverage R&D, discovery and applications with PepsiCo, discussed the company’s approach to sustainability and sustainable packaging. The company has a goal of reducing global emissions by 20% in 2030, and packaging plays a large role in that. Kulkarni also emphasized that the 20% goal is science-based. One aim is to have 100% of its packaging be recycled and recoverable. The company is looking into recycled content and bio-based polymers.
Other notes:
- PLASTICS President and CEO Bill Carteaux announced that they have a 100% waste diversion goal at NPE2018.
- PLASTICS launched a Sustainability Advisory Board, which will include members who represent the association’s key councils and committees. The goal of the Sustainability Advisory Board is to enlist a diverse group of plastics industry professionals to discuss and identify sustainability priorities in the plastics industry, which will inform projects.
Related Content
Inside the Florida Recycler Taking on NPE’s 100% Scrap Reuse Goal
Hundreds of tons of demonstration products will be created this week. Commercial Plastics Recycling strives to recycle ALL of it.
Read MoreEvolving Opportunities for Ambitious Plastics Recycler
St. Joseph Plastics grew from a simple grinding operation and now pursues growing markets in recycled PP, food-grade recycled materials, and customized post-industrial and post-consumer compounds.
Read MoreSD Polymers: 'One-Stop Solution for Mechanical Recycling'
‘Passionate’ recycler invests in people and technology to meet commitment to innovative, sustainable solutions for its processor customers.
Read MoreLooking to Run PCR on a Single Screw? Here’s What to Keep in Mind
Just drop it in and mix it up? Sorry, there’s a lot more to it than that. Here is some of what you need to consider.
Read MoreRead Next
Troubleshooting Screw and Barrel Wear in Extrusion
Extruder screws and barrels will wear over time. If you are seeing a reduction in specific rate and higher discharge temperatures, wear is the likely culprit.
Read MoreHow Polymer Melts in Single-Screw Extruders
Understanding how polymer melts in a single-screw extruder could help you optimize your screw design to eliminate defect-causing solid polymer fragments.
Read MorePeople 4.0 – How to Get Buy-In from Your Staff for Industry 4.0 Systems
Implementing a production monitoring system as the foundation of a ‘smart factory’ is about integrating people with new technology as much as it is about integrating machines and computers. Here are tips from a company that has gone through the process.
Read More