A brand-new flame-retardant Panlite PC from Teijin Chemicals Ltd.
A brand-new flame-retardant Panlite PC from Teijin Chemicals Ltd. In Japan (Teijin Kasei America is in Norcross, Ga.) is said to meet UL 94V-0 at just 1.5 mm thickness—the thinnest yet, according to the company. Teijin’s other V-0 PCs start at 2 mm. This clear resin is free of bromine or phosphorus and comes in both extrusion and injection grades. They are aimed at electrical/electronic parts, especially for LEDs and other lighting applications.