A new activator/kicker is said to be the most effective of its kind for reducing the decomposition temperature of azodicarbonamide blowing agents. Developed by South Korea’s Kum Yang Co., Ltd., and offered here by RitChem Co., Inc., Pleasantville, N.Y., Cellex BS is a zinc-based organometallic complex that imparts no odor or staining to the foam. When Cellex BS is mixed with RitChem’s Cellcom AC azo blowing agent, the blend releases gas at a temperature as low as 284 F. Cellex BS is useful with heat-sensitive substrates or for reducing plasticizer fumes. (914) 769-9110 • www.rit-chem.com