ADDITIVES: Antifog Keeps PP Sheet Clear in the Cold

New VF-P05 antifog masterbatch from Polyvel, Inc., Hammonton, N.J., is said to be highly effective in refrigerated conditions, as well as in hot environments.

Related Topics:

Related Suppliers

New VF-P05 antifog masterbatch from Polyvel, Inc., Hammonton, N.J., is said to be highly effective in refrigerated conditions, as well as in hot environments. It is aimed at sheet for food packaging and reportedly performs equally well in PP homopolymers and copolymers. VF-P05 is 30% active, a high concentration for an antifog, making it particularly cost-effective.