A new nylon 6 compound for injection molding contains 35% carbon black for excellent lightfastness.
A new nylon 6 compound for injection molding contains 35% carbon black for excellent lightfastness. PNM9404 from Techmer PM, Clinton, Tenn., can be provided in a food-grade version.