A new acetal from BASF Corp. Engineering Plastics, Wyandotte, Mich., has high melt strength for extrusion blow molding. Ultraform E3120 BM offers barrier and chemical resistance for cosmetics bottles, solvent and coolant containers, and pressure spray vessels. (800) BC-RESIN • www.plasticsportal.com/usa