BASF Corp., Florham Park, N.J., has adapted its Styrolux 3G46 styrenic block copolymer (SBC) for injection-blow and extrusion blow molding of clear hollow goods such as storage containers, decorative vessels, sports-drink bottles, and dispensers.
BASF Corp., Florham Park, N.J., has adapted its Styrolux 3G46 styrenic block copolymer (SBC) for injection-blow and extrusion blow molding of clear hollow goods such as storage containers, decorative vessels, sports-drink bottles, and dispensers. It is 30% lower in density than PVC, PETG, or PC. High impact, transparency, and exceptional gloss also reportedly make 3G46 an economical alternative for bottles with integrated handles. (973) 245-6000 • www.plasticsportal.com/usa