Carbon Nanotube-Based Epoxy Concentrates

A new line of epoxy concentrates combine several industry-standard epoxy resins with multi-wall or single-wall nanotubes or carbon nanofibers.

A new line of epoxy concentrates combine several industry-standard epoxy resins with multi-wall or single-wall nanotubes or carbon nanofibers. These products reportedly can produce composites with significant increases in electrical and thermal conductivity as well as in mechanical strength. The epoxy concentrates are the latest addition to the NanoSolve additives line from Zyvex Corp., Richardson, Texas. The company’s patented technology exfoliates and disperses carbon nano-materials and provides adhesion to the host resin.