The LHLG series air quench pelletizer from Leistritz, Somerville, N.J. mates with an extruder and enables die face cutting of pellets in air for water soluble, highly filled and foamed formulations as typically used for pharmaceutical, nutraceutical and specialty plastics products. The die is electrically heated and the flow geometry is matched with the formulation and throughput rate. The die, blades, and all contact areas are fabricated of hardened stainless, tool and carbide steels. 

Standard features include:

  • Electrically heated pelletizing die
  • Self-aligning cutter hub with replaceable blades driven by AC motor
  • Blades are manually adjusted for allowable wear
  • Stainless steel cutting chamber with sight glass and safety interlock
  • Height adjustable support cart on tracks
  • Optional chamber “misting” attachments for sticky formulations

 