Custom Hot-Runners Delivered Twice as Fast

Synventive Molding Solutions, Peabody, Mass., has revved up its fast-delivery program for Kona XP hot-runner systems so that custom systems now can be built, tested, and shipped in just two weeks.

Synventive Molding Solutions, Peabody, Mass., has revved up its fast-delivery program for Kona XP hot-runner systems so that custom systems now can be built, tested, and shipped in just two weeks. The new Kona XPress program updates a 2004 program that promised custom XP systems in four weeks.


Synventive will ship systems designed with one of six manifold shapes, four support-ring styles for nozzles, flow channels up to 25 mm diam., custom gate locations, and variable nozzle lengths and bore diameters. Valve-gate systems are available in the Kona XPress program, but not threaded nozzles, prewired systems, or complete hot-half systems with mold plates.