RTP Co., Winona, Minn., has launched a line of engineering thermoplastic compounds based on resins derived from renewable resources.
RTP Co., Winona, Minn., has launched a line of engineering thermoplastic compounds based on resins derived from renewable resources. The 15 initial products are based on polyamide, polyester, or polylactic acid (PLA). Polyamide and polyester grades are offered with glass fiber, antistatic/ESD protection, halogen-free flame retardant, and/or PTFE lubrication. PLA comes with impact modifier or blended with PC, ABS, or PMMA.