The Stanyl nylon 46 line from DSM Engineering Plastics, Evansville, Ind., has been expanded with a new high-flow series called Stanyl Super Flow. The first grade, Stanyl 46SF5030, is aimed at small electronic connectors with high pin counts (up to 100 or more), walls as thin as 0.06 mm, and pitch values well below 0.3 mm. The 30% glass-filled product is said to have exceptional ductility and weld-line strength. In lead-free soldering, it resists blistering in thin sections and retains its high mechanical properties. Stanyl 46SF5030 is rated UL 94V-0 at 0.4 mm and is RoHS compliant.