R&D Tool and Engineering, Lee's Summit, Mo., has introduced a new quick-change lower blow mold assembly for one-step stretch-blow molding machines such as those from Nissei and Aoki.
R&D Tool and Engineering, Lee's Summit, Mo., has introduced a new quick-change lower blow mold assembly for one-step stretch-blow molding machines such as those from Nissei and Aoki. The system reduces the number of parts and cavitation-dependent components. It is claimed to reduce tool changeover time by 50%. The design incorporates the blow cavities into a monoblock that is mounted on a universal backplate with patented quick-disconnect couplings.