Merquinsa in Spain (U.S. office in Seabrook, N.H.) has expanded its range of Pearlthane ECO TPUs made with renewable plant-based ingredients to now include the world’s first polyether “bio TPU.” These grades will have up to 60% renewable content. (603) 474-0971 • www.merquinsa.comMerquinsa North America Inc. 34 Folly Mill Road Seabrook, NH 03874 Phone (603) 474-0971 Fax (603) 474-0972