A new series of glass-filled PEEK grades from Victrex USA Inc., Greenville, S.C., are FDA-compliant for food-processing and related industrial applications.

Related Suppliers

A new series of glass-filled PEEK grades from Victrex USA Inc., Greenville, S.C., are FDA-compliant for food-processing and related industrial applications. Like unfilled grades, the glass-filled materials comply with the requirements of the 21CFR 177.2415 standard. Targeted applications include bearings, seals, precision cutting blades, and energy-efficient pumps.