StarRov 908 is a new direct-wound fi berglass roving for pultrusion from Johns Manville Engineered Products, Waterville, Ohio.
StarRov 908 is a new direct-wound fi berglass roving for pultrusion from Johns Manville Engineered Products, Waterville, Ohio. It has surface sizings compatible with unsaturated polyester, vinyl ester, and epoxy resins. The new roving is said to reduce fuzz and strand breaks during pultrusion operations. It comes in 1200 to 9600 tex. Tel: (800) 554-4830 . www.jm-reinforcement.com