A new non-halogenated copolyester TPE has been launched by DSM Engineering Plastics, Evansville, Ind., as an alternative to PVC for cable insulation in consumer electronics. Arnitel XG meets the UL VW1 specification, widely regarded as the industry standard. It fully meets flammability criteria for cable insulation, is safely recyclable, and resists household cleaning substances. It also has a soft touch and excellent colorability for improved aesthetics. (812) 435-7500 • www.dsmep.com