Center runners, gates with small inserts, and other mold areas with limited access for cooling may benefit from the new Inlet Cascade from Progressive Components International Corp., Wauconda, Ill.
Center runners, gates with small inserts, and other mold areas with limited access for cooling may benefit from the new Inlet Cascade from Progressive Components International Corp., Wauconda, Ill. This new brass fitting combines the “in” waterline with a cascade to cool a targeted area. The component reduces machining required in the insert, can be used in high-temperature molds, and is available with a wide range of cascade tube options. Tel: (847) 487-1000 • www.procomps.com
Progressive Components
235 Industrial Dr. Wauconda, IL 60084-1078
Phone (800) 269-6653 Fax (800) 462-6653