A new semi-permanent mold release from Axel Plastics Research Laboratories, Woodside, N.Y., is aimed at production of sanitary ware and other high-gloss parts. Xtend 830 is a solvent-based release that is applied to the mold and then wiped off, leaving a glossy, streak-free surface. Testing has shown gloss improvement from 88 to 94 at 20°, according to the company. Molders of sanitary ware who need to reposition sink bowls or other elements between molding cycles are able to wipe the mold release over dirty areas to clean up clay and wax marks. No cleaners or strippers are needed to prepare the mold for additional production. (718) 672-8300 • www.axelplastics.com