A highly amorphous PP homopolymer is said to produce films with exceptional stretchability.
A highly amorphous PP homopolymer is said to produce films with exceptional stretchability. Grade FF025F is the newest specialty film grade from Sunoco Chemicals, Philadelphia. It is offered in a variety of melt flows for BOPP and cast film. Business director Carmen Melillo describes this highxylene-solubles resin as “an excellent all-purpose grade.” (215) 977-3142 • www.sunocoinc.com