A new semi-flexible, cycloaliphatic epoxy from Huntsman Advanced Materials, The Woodlands, Texas, is used to mold sheds for outdoor electrical insulators in medium- to high-voltage applications. Araldite S-HCEP is hydrophobic and provides good tracking and erosion resistance and good water-diffusion breakdown strength. The system has a 1:1 mix ratio, so it can be dispensed with equipment used for liquid silicone rubber. It needs no stirring, degassing, or preheating and adheres well to composite rods without a primer. (888) 564-9318 • www.huntsman.com/advanced_materials