INJECTION MOLDING: Competitively Priced Robots From China

Extensive line of servo and hybrid linear robots and pickers.

Related Topics:

Related Suppliers

Visitors to NPE2015, March 23-27 in Orlando, Fla., will have an opportunity to acquaint themselves with an extensive line of Cartesian robots available from a relatively new U.S. distributor. Absolute Robot, Inc., Worcester, Mass., was founded in 2013 as a sister company to Absolute Haitian (a supplier of Chinese injection presses) and other members of the Absolute Group. It markets robots from Well-Lih Robotics in China. Established in 2003, Well-Lih produces around 6000 robots annually.

Products configured for the North American market include a variety of full-servo robots for presses from 80 to 3300 tons, including models with telescoping arms and dual arms. There are also hybrid servo/pneumatic models for presses from 50 to 530 tons, pneumatic pickers for 50-470 tons, and a variety of control pendants, including a touchscreen, full-servo model.