Beck Automation of Switzerland says it will exhibit for the first time at the K 2010 show in-mold labeling of a clear, thin-wall PS cup in which the labeling is visible from both inside and outside.
Beck Automation of Switzerland says it will exhibit for the first time at the K 2010 show in-mold labeling of a clear, thin-wall PS cup in which the labeling is visible from both inside and outside. The two-side-printed labels come from Viappiani in Segrete, Italy. Beck’s robot system will place the labels in four cavities in a Netstal Elion 1750-840 machine with a mold from Glaroform of Nafels, Switzerland. Cycle time will be 3.0 sec.
+41 44 751 84 44 • beck-automation.com