WEB EXCLUSIVE: Durr Marketing Associates, Inc. and its affiliate Azalea Color Co., both of Pittsburgh, are the new exclusive North American distributor for additives from SABO SRL of Levate, Italy.

WEB EXCLUSIVE: Durr Marketing Associates, Inc. and its affiliate Azalea Color Co., both of Pittsburgh, are the new exclusive North American distributor for additives from SABO SRL of Levate, Italy. Durr and Azalea will sell SABO’s full line of HALS UV stabilizers, antioxidants, antistats, and antifog agents. Previously, the two companies had offered SABO Stab UV 119, a HALS previously offered by Ciba as Chimassorb 119 FL. Ciba was required to divest the product to satisfy competition concerns in the HALS market resulting from Ciba’s acquisition by BASF. (800) 245-2877 * www.azaleacolor.com