A new high-speed rotary extrusion blow molder from R&B Plastics Machinery, Saline, Mich., boasts wide platens for greater output. The Rotary 8-15 model has 32 x 18 in. platens, considerably larger than R&B's other rotary models. The eight-station machine comes with up to nine parisons and coex capability for up to six layers. The machine can produce containers up to 2.5 gal with a calibrated neck finish. The unit features a patented onboard XY blowpin design for neck-finish calibration, and an open index station allows for highly accurate label placement in IML applications. Annual output ranges up to 129 million containers.