WEB EXCLUSIVE: Pelco Tool & Mold, Inc., Glendale Heights, Ill., has acquired a license from Husky Injection Molding Systems Ltd., Bolton, Ont., to produce closure molds utilizing Husky’s Rotating Ratchet Ring (RRR) technology. “RRR” molds reportedly have shown 25% shorter cycle times than conventional unscrewing closure molds with rotating cores, and require less maintenance as well.(630) 871-1010 • pelcotool.com(905) 951-5000 • husky.caHusky Injection Molding Systems 500 Queen St.
WEB EXCLUSIVE: Pelco Tool & Mold, Inc., Glendale Heights, Ill., has acquired a license from Husky Injection Molding Systems Ltd., Bolton, Ont., to produce closure molds utilizing Husky’s Rotating Ratchet Ring (RRR) technology. “RRR” molds reportedly have shown 25% shorter cycle times than conventional unscrewing closure molds with rotating cores, and require less maintenance as well.
(630) 871-1010 • pelcotool.com
(905) 951-5000 • husky.ca
Husky Injection Molding
Systems
500 Queen St. South Bolton L7E 5S5, Ontario, Canada
Phone (905) 951-5000