The Complet line of long-fiber reinforced thermoplastic (LFRT) pellets from PlastiComp LLC, Winona, Minn., now is available with color, impact modifier, and/or other additives. This "single-pellet" solution eliminates the need to blend in color or additive masterbatches and the subsequent risk of the blend segregating during transport and conveying. PlastiComp offers pellets with lengths from 10 to 12 mm and also 6-mm pellets for small-part molding. Tel: (507) 454-4334 . www.plasticomp.com