A new 26% long-glass acetal copolymer from Ticona Engineering Polymers, Florence, Ky., is aimed at structural automotive and appliance parts, as well as gears.
A new 26% long-glass acetal copolymer from Ticona Engineering Polymers, Florence, Ky., is aimed at structural automotive and appliance parts, as well as gears. Hostaform LGC90QX reportedly offers a combination of exceptional impact resistance, inherent lubricity, and strong fuel and chemical resistance for sunroof systems, auto seating systems, high-load gears, and other industrial parts. (800) 526-4960 • www.ticona.com