Ticona Engineering Polymers, Florence, Ky., has developed a low-chlorine version of Fortron PPS that meets eco-compliant demands for electrical and electronics components.
Ticona Engineering Polymers, Florence, Ky., has developed a low-chlorine version of Fortron PPS that meets eco-compliant demands for electrical and electronics components. Enhanced polymerization and compounding technology reduces the chlorine concentration of Fortron 1140A66 to below 900 ppm without loss of mechanical properties. The material also meets the UL 94V-0 flammability rating without the use of flame retardants. (800) 526-4960 • www.ticona.com
Ticona
8040 Dixie Hwy. Florence, KY 41042-2904
Phone (859) 525-4740 Fax (859) 525-4770