A new line of flat dies and feedblocks is being introduced into North America as TruFlow by Maag Pump Systems, Charlotte, N.C. The TruFlow dies are built in China using either German or Japanese P20 tool steel and are expected to be at least 20% less expensive than comparable dies built here. Maag has worked with the Chinese supplier on other products. Maag is storing a full inventory of standard dies and spare parts in the U.S. and is servicing the dies in Charlotte. Maag will also contract for specialized refurbishing, like replating, in North America, as well. Maag’s TruFlow dies come in standard and custom inch sizes from 18 in. to 18 ft wide for foam, film, sheet, up to 9-layer coextrusion, and PVC siding. (704) 716-9000 • www.maag.com
Maag Pump Systems Textron Inc.
1500 Continental Blvd. #Z Charlotte, NC 28273
Phone (704) 716-9000 Fax (704) 716-9001