A new high-temperature lubricant for liquid silicone rubber or other thermoset molds, and a new solvent for cleaning between lubrication cycles, come from Alba Enterprises Inc., Rancho Cucamonga, Calif.
A new high-temperature lubricant for liquid silicone rubber or other thermoset molds, and a new solvent for cleaning between lubrication cycles, come from Alba Enterprises Inc., Rancho Cucamonga, Calif. The grease is stable at up to 572 F. Alba's new cleaning solvent removes grease, oil, resin, or dirt prior to lubrication of mold or machine components. Tel: (909) 941-0600 . www.albaent.com