MATERIALS: Blow-Moldable TPV for Automotive and Beyond

This 90 Shore A hardness blow-moldable TPV can be optimized with specific softness needed in a variety of parts.

Related Suppliers

APS Elastomers, Romulus, Mich., has developed a blow-moldable TPV for automotive as well as other applications. The engineered Viprene TPV can be used in hollow boots, bellows and duct applications as well as is in similar applications in snowmobiles, ATVs, off-road vehicles and industrial equipment. It has a Shore A hardness of 90, and can be optimized with specific softness needed in a variety of parts. (734) 710-6700 • apstpe.com