MATERIALS: Halogen-Free TPVs for Power Cords/Cables

WEB EXCLUSIVE: A new line of halogen-free flame-retardant TPVs for consumer and industrial electronic power cords and auxiliary cables is available from Alliance Polymer and Services, LLC, Romulus, Mich.

Related Suppliers

WEB EXCLUSIVE: A new line of halogen-free flame-retardant TPVs for consumer and industrial electronic power cords and auxiliary cables is available from Alliance Polymer and Services, LLC, Romulus, Mich. Positioned as halogen- and phthalate-free alternatives to flexible PVC, Viprene V85A-27U-BLK was developed specifically for power plugs, charger cables, electronic power cords, auxiliary cables, and ribbon wire. These grades reportedly are easy to process and have good surface quality.